GA-2100D
Herchy
| Cothrom: | |
|---|---|
| Meud: | |
Deuchainn: A: B co-mheas de 1: 1, 130 ℃ x 5min x 15MPa.
| Paramadairean toraidh | |||||||
| Bathar | GA-2100D | GA-2105D | GA-2110d | GA-2115D | GA-2120D | GA-2125D | |
| Coltas | Tar-shoilleir | ||||||
| Slaodachd (Pas) |
A: 1.0 B:1.0 |
A: 4.0 B: 4.0 |
A: 3.0 B: 3.0 |
A: 3.5 B: 3.5 |
A: 4.6 B: 4.3 |
A: 4.5 B: 4.5 |
|
| cruas (CladachA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Dlùths (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Neart tensile (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Leudachadh (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Neart deòir (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|