GA-2100D
Herchy
| Beschikbaarheid: | |
|---|---|
| Aantal: | |
Test: A:B-verhouding van 1:1, 130℃ x 5min x 15MPa.
| Productparameters | |||||||
| Product | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Verschijning | Doorschijnend | ||||||
| Viscositeit (Pa.s) |
EEN:1.0 B:1,0 |
A:4,0B :4,0 |
A:3,0B :3,0 |
A:3,5 B:3,5 |
A:4,6 B:4,3 |
A:4,5 B:4,5 |
|
| Hardheid (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Dichtheid (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Treksterkte (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Verlenging (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Scheursterkte (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|