Past viskoziteli LSR (LSR)

Ilova: silikon inson niqobi, silikon sun'iy organlar, silikon modellar va shakarlamalar, shokolad, pechene, kek va boshqalarning yuqori simulyatsiya qoliplarini ishlab chiqarish uchun javob beradi.
Asosiy xususiyatlar: yaxshi suyuqlik, osonlik bilan disk raskadrovka
  • GA-2100D

  • Herchi

Mavjudligi:
Miqdor:

Sinov: A:B nisbati 1:1, 130℃ x 5min x 15MPa.


Mahsulot parametrlari
Mahsulot GA-2100D GA-2105D GA-2110D GA-2115D GA-2120D GA-2125D
Tashqi ko'rinish Shaffof

Yopishqoqlik (Pa.s)

Javob: 1.0

B: 1,0

A: 4,0

B: 4,0

A: 3,0

B: 3,0

A: 3,5

B: 3,5

A: 4,6

B: 4,3

A: 4,5

B: 4,5
Qattiqlik (ShoreA) 0 5 10 15
20
25
Zichlik (g/sm3) 1.10
1.10
1.12
1.12 1.10
1.12
Kuchlanish kuchi (MPa) 0.4
2.5
3.0
4.0
6.0
6.0
Uzayish (%) 500 500 600 550 600
600
Yirilish kuchi (kN/m) 1.5 8 7
8 11
14











Oldingi: 
Keyingisi: 

TEZKOR havolalar

MAHSULOTLARIMIZ

BOG'LANISH UCHUN MA'LUMOT

Qo'shish: №33, 159-ko'cha, Taiye yo'li, Fengxian tumani, Shanxay
Tel / WhatsApp / Skype: +86 15221953351
Mualliflik huquqi     2023 Shanghai Herchy Rubber Co., Ltd. Sayt xaritasi |   Maxfiylik siyosati | Qo'llab-quvvatlash Leadong.