GA-2100D
Herčijs
| Pieejamība: | |
|---|---|
| Daudzums: | |
Tests: A:B attiecība 1:1, 130℃ x 5min x 15MPa.
| Produkta parametri | |||||||
| Produkts | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Izskats | Caurspīdīgs | ||||||
| Viskozitāte (Pa.s) |
A:1.0 B:1,0 |
A: 4,0 B: 4,0 |
A: 3,0 B: 3,0 |
A: 3,5 B: 3,5 |
A: 4,6 B: 4,3 |
A: 4,5 B: 4,5 |
|
| Cietība (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Blīvums (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Stiepes izturība (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Pagarinājums (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Plīsuma izturība (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|