GA-2100D
Herçi
| Elýeterlilik: | |
|---|---|
| mukdary: | |
Synag: A: B gatnaşygy 1: 1, 130 ℃ x 5min x 15MPa.
| Önümiň parametrleri | |||||||
| Haryt | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Daş görnüşi | Düşünjeli | ||||||
| Iscapyşmazlyk (Pa.s) |
J: 1.0 B: 1.0 |
J: 4.0 B: 4.0 |
J: 3.0 B: 3.0 |
J: 3.5 B: 3.5 |
J: 4.6 B: 4.3 |
J: 4.5 B: 4.5 |
|
| Gatylyk (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Dykyzlygy (g / cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Dartyş güýji (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Uzalma (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Göz ýaşyň güýji (kN / m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|