GA-2100D
Herchy
| Ketersediaan: | |
|---|---|
| Kuantitas: | |
Tes: Rasio A:B 1:1, 130℃ x 5 menit x 15MPa.
| Parameter produk | |||||||
| Produk | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Penampilan | Tembus cahaya | ||||||
| Viskositas (Pa.s) |
J:1.0 B:1.0 |
J:4.0 B:4.0 |
J:3.0 B:3.0 |
J:3.5 B:3.5 |
J:4.6 B:4.3 |
J:4.5 B:4.5 |
|
| Kekerasan (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Kepadatan (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Kekuatan tarik (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Pemanjangan(%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Kekuatan sobek (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|