GA-2100D Fotoen
Herchy
| Verfügbarkeet: | |
|---|---|
| Quantitéit: | |
Test: A:B Verhältnis vun 1:1, 130 ℃ x 5min x 15MPa.
| Produit Parameteren | |||||||
| Produit | GA-2100D Fotoen | GA-2105D Fotoen | GA-2110D Fotoen | GA-2115D Fotoen | GA-2120D Fotoen | GA-2125D Fotoen | |
| Ausgesinn | Duerchsichteg | ||||||
| Viskositéit (Pa.s) |
A: 1,0 B: 1,0 |
A: 4,0 B: 4,0 |
A: 3,0 B: 3,0 |
A: 3,5 B: 3,5 |
A: 4,6 B: 4,3 |
A: 4,5 B: 4,5 |
|
| Hardness (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Dicht (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Tensile Stäerkt (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Verlängerung (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Tréinekraaft (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|