GA-2100D jedhamuun beekama
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay'ina: | |
Qormaata: Reeshiyoo A:B 1:1, 130°C x 5min x 15MPa.
| Parameetaroota oomishaa | |||||||
| Oomisha | GA-2100D jedhamuun beekama | GA-2105D jedhamuun beekama | GA-2110D jedhamuun beekama | GA-2115D jedhamuun beekama | GA-2120D jedhamuun beekama | GA-2125D jedhamuun beekama | |
| Mul'ina | Kan ifa ta’e | ||||||
| Viskoositii(Pa.s) 1.1. |
Y:1.0 B:1.0 |
A:4.0 B:4.0 jechuun ni danda’ama |
A:3.0 B:3.0 jechuun ni danda’ama |
A:3.5 B:3.5 |
A:4.6 B:4.3 |
A:4.5 B:4.5 |
|
| Jabina (ShoreA) . | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Dandeettii(g/cm3) . | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Cimina harkisaa (MPa) . | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Dheersuu(%) . | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Jabina ciccituu (kN/m) . | 1.5 | 8 | 7 |
8 | 11 |
14 |
|