GA-2100D
Herchy
| Kasedhiyan: | |
|---|---|
| Jumlah: | |
Tes: rasio A:B 1:1, 130 ℃ x 5min x 15MPa.
| Parameter produk | |||||||
| produk | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Penampilan | Tembus | ||||||
| Viskositas (Pa) |
A: 1.0 B: 1.0 |
A:4.0 B:4.0 |
A: 3.0 B: 3.0 |
A:3.5 B:3.5 |
A:4.6 B:4.3 |
A:4.5 B:4.5 |
|
| Kekerasan (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Kapadhetan (g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Kekuatan tarik (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Elongasi (%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Kekuwatan sobek (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|