LSR a ɛnyɛ den pii (LSR) .

Dwumadi: ɛfata ma silicone onipa akataso, silicone artificialorgans, silicone nhwɛsode, ne soro simulation nkuku a candy nnuaba, chocolate,biscuits, keeki ne nea ɛkeka ho.
Nneɛma atitiriw: fluidity pa, ɛnyɛ den sɛ wobɛpopa
  • GA-2100D na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Availability:
Quantity:

Sɔhwɛ: A: B nsusuwii a ɛyɛ 1:1, 130°C x 5min x 15MPa.


Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-2100D na ɛwɔ hɔ GA-2105D na ɛwɔ hɔ GA-2110D na ɛwɔ hɔ GA-2115D na ɛwɔ hɔ GA-2120D na ɛwɔ hɔ GA-2125D na ɛwɔ hɔ
Mmaeɛ Ɛyɛ nea ɛyɛ translucent

Nsuo a ɛyɛ den(Pa.s) .

A:1.0

B:1.0 na ɛwɔ hɔ

A:4.0

B:4.0 na ɛwɔ hɔ

A:3.0

B:3.0 na ɛwɔ hɔ

A:3.5

B:3.5 na ɛwɔ hɔ

A:4.6

B:4.3 na ɛwɔ hɔ

A:4.5

B:4.5 na ɛwɔ hɔ
Nneɛma a ɛyɛ den (Shor 0 5 10 15
20
25
Nsuo a ɛyɛ den(g/cm3) . 1.10
1.10
1.12
1.12 1.10
1.12
Ahoɔden a wɔde twe ade (MPa) . 0.4
2.5
3.0
4.0
6.0
6.0
Ntrɛwmu(%) . 500 500 600 550 600
600
Ahoɔden a ɛtetew mu (kN/m) . 1.5 8 7
8 11
14











Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.