GA-2100D ƒe agbalẽa
Herchy .
| Availability: | |
|---|---|
| Quantity: | |
Dodokpɔ: A: B ƒe xexlẽme si nye 1:1, 130°C x 5min x 15MPa.
| Adzɔnuwo ƒe nɔnɔmetatawo . | |||||||
| Nu si wowɔ | GA-2100D ƒe agbalẽa | GA-2105D ƒe agbalẽa | GA-2110D ƒe agbalẽa | GA-2115D ƒe agbalẽa | GA-2120D ƒe agbalẽa | GA-2125D ƒe agbalẽa | |
| Dzedzeme | Translucent . | ||||||
| Viscosity(Pa.s) ƒe ʋeʋẽ lilili . |
A:1.0 B:1.0 |
A:4.0 B:4.0 |
A:3.0 B:3.0 |
A:3.5 B:3.5 |
A:4.6 B:4.3 |
A:4.5 B:4.5 |
|
| Sesẽ (Shorea) . | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Density(G/CM3) . | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Tensile ƒe ŋusẽ (MPA) . | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Elongation(%) . | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Aɖatsiŋusẽ (kn/m) . | 1.5 | 8 | 7 |
8 | 11 |
14 |
|