GA-11×3
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175°C x 5min x 15MPa.
| Product parameters | ||||||
| Product | GA-1133 | GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
| Appearance | Translucent | |||||
| Williamplasticity | 115 | 150 | 205 | 240 | 280 | 310 |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 | 80 |
| Density(g/cm3) | 1.10 | 1.12 | 1.16 | 1.19 | 1.22 | 1.22 |
| Tensilestrength (MPa) | 7.5 | 7.5 | 9 | 8.5 | 8.5 | 7.5 |
| Elongation(%) | 700 | 500 | 450 | 400 | 300 | 200 |
| Tearstrength (kN/m) | 16 | 20 | 20 | 20 | 20 | 16 |