GA-11×3 rehegua
Herchy rehegua
| Ojeguereko: | |
|---|---|
| Cantidad: 1.1. | |
Prueba: 1% agente curador (50% pasta DBPMH goma de silicona-pe), 175°C x 5min x 15MPa.
| Umi parámetro producto rehegua | ||||||
| Mba'eapopyre | GA-1133 rehegua |
GA-1143 rehegua | GA-1153 rehegua | GA-1163 rehegua | GA-1173 rehegua | GA-1183 rehegua |
| Ojehechaháicha | Translúcido rehegua | |||||
| Williamplasticidad rehegua |
115 |
150 |
205 |
240 |
280 |
310 |
| Dureza (ShoreA) rehegua . |
30 |
40 |
50 |
60 |
70 |
80 |
| Densidad(g/cm3) rehegua. | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Resistencia a la tracción (MPa) rehegua . |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
| Alongación(%) rehegua . | 700 |
500 |
450 |
400 |
300 |
200 |
| Tesay mbarete (kN/m) . | 16 |
20 |
20 |
20 |
20 |
16 |