GA-11×3
Herchy
| Ku kumeka: | |
|---|---|
| Nhlayo: . | |
Xikambelo: 1% wa xiaki xo horisa (50% wa paste ya DBPMH eka silicone gum), 175°C x 5min x 15MPa.
| Tipharamitha ta Xiendliwa . | ||||||
| Ximakiwa | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
| Xivumbeko | Ku vonakala loku vonakaka | |||||
| WilliamPlasticity . |
115 |
150 |
205 |
240 |
280 |
310 |
| Ku nonoka (ShoreA) . |
30 |
40 |
50 |
60 |
70 |
80 |
| Ku tsindziyela(g/cm3) . | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Ku tiya ka ku tsana (MPa) . |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
| Ku leha(%) . | 700 |
500 |
450 |
400 |
300 |
200 |
| Ku tiya ka mihloti (kN/m) . | 16 |
20 |
20 |
20 |
20 |
16 |