ꯖꯤ.ꯑꯦ.-꯱꯱×꯳
ꯍꯔꯆꯤ꯫
| ꯐꯪꯒꯗꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: ꯱. | |
ꯇꯦꯁ꯭ꯠ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ 1% (ꯁꯤꯂꯤꯀꯣꯟ ꯒꯃꯗꯥ DBPMHꯒꯤ 50% ꯄꯦꯁ꯭ꯠ), 175°C x 5min x 15MPa꯫
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | ||||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯱꯱꯳꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ |
ꯖꯤ.ꯑꯦ.-꯱꯱꯴꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯱꯱꯵꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯱꯱꯶꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯱꯱꯷꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯱꯱꯸꯳ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯇ꯭ꯔꯥꯟꯁꯂꯨꯁꯦꯟꯇ ꯑꯣꯏꯕꯥ꯫ | |||||
| ꯎꯏꯂꯤꯌꯥꯃꯞꯂꯥꯁ꯭ꯇꯤꯁꯤꯇꯤ ꯂꯩꯕꯥ꯫ |
115 |
150 |
205 |
240 |
280 |
310 |
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. |
30 |
40 |
50 |
60 |
70 |
80 |
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| ꯇꯦꯟꯁꯥꯏꯂꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
| ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. | 700 |
500 |
450 |
400 |
300 |
200 |
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯂꯩꯕꯥ꯫ | 16 |
20 |
20 |
20 |
20 |
16 |