GA-11×3
Herchy
| Helitaanka: | |
|---|---|
| Tirada: | |
Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka), 175°C x 5min x 15MPa.
| Xuduudaha alaabta | ||||||
| Alaabta | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
| Muuqashada | Translucent | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
310 |
| Adag ( ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Cufnaanta (g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Xoog adkaysi (MPa) |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
| Dheeraynta(%) | 700 |
500 |
450 |
400 |
300 |
200 |
| Xoogga ilmada (kN/m) | 16 |
20 |
20 |
20 |
20 |
16 |