Ga-11 × 3 intego rusange silicone reberi yo kubumba (HCR)

Gusaba: Utubuto busanzwe, kashe hamwe nibindi bicuruzwa bikunze kugaragara.
o Ibiranga ibyingenzi: Kwihangana neza, gahunda nziza cyane 小 ty, kurenga ku byemezo bya
rohs, kugera kuri FHS, na FDA.
  • Ga-11 × 3

  • Herchy

Kuboneka:
ubwinshi:

Ikizamini: 1% yo gukiza agent (50% paste ya DBPMH muri Bam Silicone), 175 ° C x 5min x 15MPA.


Ibipimo by'ibicuruzwa
Ibicuruzwa Ga-1133
Ga-1143 Ga-1153 Ga-1163 Ga-1173 Ga-1183
Isura Bisobanutse
WilliamPlastity
115
150
205
240
280
310
Gukomera (Shorea)
30
40
50
60
70
80
Ubucucike (G / CM3) 1.10
1.12
1.16
1.19
1.22
1.22
Uburebure bwa Tenilestre (MPA)

7.5
7.5
9
8.5
8.5
7.5
Kurambagiza (%) 700
500
450
400
300
200
Uburebure bwa Teardre (KN / M) 16
20
20
20
20
16



Mbere: 
Ibikurikira: 

Ihuza ryihuse

Ibicuruzwa byacu

Amakuru Yamakuru

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Tayiye, Akarere ka FEGXIAN, Shanghai
Tel / Whatsapp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co, Ltd. SiteMap |   Politiki Yibanga | Inkunga by Linang.