GA-11×3 Silikoni ka lastikuw caman sɔrɔli kama (HCR) .

A kɛcogo: Butɔn gansanw, sigilanw ani fanga sɔrɔcogo kɔrɔlen wɛrɛw.
o Fɛn kolomaw: Resilience ɲuman, processab小ty ɲumanba, tɛmɛ
Rohs, Reach, ani FDA ka tiɲɛni kan.
  • GA-11×3.

  • Herchy .

Sɔrɔli:
Hakɛ:

Kɔrɔbɔli: 1% furakɛli fura (50% DBPMH pasti silikoni na), 175°C x 5min x 15MPa.


Product Paramɛtɛrɛw .
Ka kɛ GA-1133 .
GA-1143 . GA-1153 . GA-1163 . GA-1173 . GA-1183 .
Yecogo translucent .
WilliamPlasticity .
115
150
205
240
280
310
Gɛlɛya (Shoaa) .
30
40
50
60
70
80
density(G/CM3) . 1.10
1.12
1.16
1.19
1.22
1.22
Tensilestrength (MPa) .

7.5
7.5
9
8.5
8.5
7.5
elongation(%) . 700
500
450
400
300
200
Ɲɛgɛnɛsiraw (KN/M) . 16
20
20
20
20
16



Tɛmɛnen: 
Nata: 

Link teliyalenw .

An ka fɛn dilannenw .

Kunnafoni minnu bɛ sɔrɔ .

Fàra o kan: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap . |   Kunnafoni-falen-falen sariyaw | dɛmɛ don ni . Leadong ..