Prawf: 1% o'r asiant halltu (past 50% o dbpmh mewn gwm silicon), 175 ° C x 5 munud x 15mpa.
Paramedrau Cynnyrch | ||||||
Nghynnyrch | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
Ymddangosiad | Tryloyw | |||||
Williamplasticity |
115 |
150 |
205 |
240 |
280 |
310 |
Caledwch (Shorea) |
30 |
40 |
50 |
60 |
70 |
80 |
Dwysedd (g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
Tensilestrength (MPA) |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
Elongation (%) | 700 |
500 |
450 |
400 |
300 |
200 |
DEARSTRENGTH (kN/M) | 16 |
20 |
20 |
20 |
20 |
16 |
Prawf: 1% o'r asiant halltu (past 50% o dbpmh mewn gwm silicon), 175 ° C x 5 munud x 15mpa.
Paramedrau Cynnyrch | ||||||
Nghynnyrch | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
Ymddangosiad | Tryloyw | |||||
Williamplasticity |
115 |
150 |
205 |
240 |
280 |
310 |
Caledwch (Shorea) |
30 |
40 |
50 |
60 |
70 |
80 |
Dwysedd (g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
Tensilestrength (MPA) |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
Elongation (%) | 700 |
500 |
450 |
400 |
300 |
200 |
DEARSTRENGTH (kN/M) | 16 |
20 |
20 |
20 |
20 |
16 |