Ga-11 × 3
G'amgin
Mavjudlik: | |
---|---|
miqdor: | |
Sinov: davolash vositasining 1% (Dbpmh s kremnitonida 50% past), 175 ° C x 5 min x 15mpa.
Mahsulot parametrlari | ||||||
Mahsulot | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
Tashqi ko'rinish | Shaffof | |||||
WilliaMplastikligi |
115 |
150 |
205 |
240 |
280 |
310 |
Qattiqlik (Shorea) |
30 |
40 |
50 |
60 |
70 |
80 |
Zichlik (g / sm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
Kesilestreng (MPA) |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
Cho'zish (%) | 700 |
500 |
450 |
400 |
300 |
200 |
Ko'z yoshlar darajobang uzunligi (kn / m) | 16 |
20 |
20 |
20 |
20 |
16 |
Sinov: davolash vositasining 1% (Dbpmh s kremnitonida 50% past), 175 ° C x 5 min x 15mpa.
Mahsulot parametrlari | ||||||
Mahsulot | GA-1133 |
GA-1143 | GA-1153 | GA-1163 | GA-1173 | GA-1183 |
Tashqi ko'rinish | Shaffof | |||||
WilliaMplastikligi |
115 |
150 |
205 |
240 |
280 |
310 |
Qattiqlik (Shorea) |
30 |
40 |
50 |
60 |
70 |
80 |
Zichlik (g / sm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
Kesilestreng (MPA) |
7.5 |
7.5 |
9 |
8.5 |
8.5 |
7.5 |
Cho'zish (%) | 700 |
500 |
450 |
400 |
300 |
200 |
Ko'z yoshlar darajobang uzunligi (kn / m) | 16 |
20 |
20 |
20 |
20 |
16 |