GA-2041WY Fire-retardant fluid silicone reberi yo gutwikira (LSR)

Gushyira mu bikorwa: bikwiranye nurupapuro rwerekana ibicuruzwa, ibirahuri bya fibre bifunze, ibicuruzwa hamwe na sponge. 
Ibyingenzi byingenzi: guhuza gukomeye hamwe na substrate, umuvuduko ukiza byihuse, ibyiza ce 「amiceffect.
  • GA-2041WY

  • Herchy

Kuboneka:
Umubare:

Ikizamini: Ikigereranyo cya A / B kirashobora guhinduka, 130 ° C x 5min x 15MPa


Ibipimo byibicuruzwa
Ibicuruzwa GA-2041WY GA-2051WY GA-2061WY GA-2071WY
Kugaragara Icyatsi kibisi Icyatsi kibisi Icyatsi cyijimye Icyatsi kibisi
A / Bratio
2: 100 2: 100 1: 1 2: 100
Viscosity (Pa.s)
14-20 140-160 70-90 140-160
Gukomera (ShoreA) 45 50
65
70
Ubucucike (g / cm3)

1.3

1.36 1.6 1.5
Imbaraga zingana (MPa) 2.5
3.0
3.0
3.0
Kurambura (%) 200 300 170 140
Amarira amarira (kN / m) 7 7 7
8
Icyiciro cya flame
UL94V-0 UL94V-0 UL94V-0 UL94V-0









Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.