GA-2041WY Ignis retardans liquor silicone Flexilis efficiens (LSR)

Applicatio: apta ad producendumsilicone linteum, fibra vitrea efficiens, producta spongia coatinganda. 
Key lineamenta: valida coniunctio cum subiectis, celeritas sanans ieiunium, bonum ce「amiceffectus.
  • GA-2041WY

  • Herchy

Availability:
Quantity:

Test: A/B ratio aptabilis, 130°C x 5min x 15MPa


Product parametri
Productum GA-2041WY GA-2051WY GA-2061WY GA-2071WY
Aspectus Lux griseo Lux griseo griseo Lux griseo
A/Bratio
2:100 2:100 1, 1; 2:100
Viscositas (Pa.s)
14-20 140-160 70-90 140-160
Duritia (ShoreA) 45 50
65
70
Densitas (g/cm3)

1.3

1.36 1.6 1.5
Roboris distrahentes (MPa) 2.5
3.0
3.0
3.0
Prolongatio(%) 200 300 170 140
Robur scindere (kN/m) 7 7 7
8
Flamma classis
UL94V-0 UL94V-0 UL94V-0 UL94V-0









Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.