GA-2041WY
Herchy
Beskikberens: | |
---|---|
kwantiteit: | |
Test: A / B-ferhâlding is ferstelber, 130 ° C X 5MIN X 15MPA
Produktparameters | |||||
Produkt | GA-2041WY | GA-2051wY | GA-2061wy | GA-2071wY | |
Ferskining | Ljocht griis | Ljochtgriis | Donker griis | Ljochtgriis | |
A / Bratio |
2: 100 | 2: 100 | 1: 1 | 2: 100 | |
Viscosity (PA.S) |
14-20 | 140-160 | 70-90 | 140-160 | |
Hurdens (Shorea) | 45 | 50 |
65 |
70 |
|
DENSITY (G / CM3) | 1.3 |
1.36 | 1.6 | 1.5 | |
Tensile krêft (MPA) | 2.5 |
3.0 |
3.0 |
3.0 |
|
ELONGATION (%) | 200 | 300 | 170 | 140 | |
Slachterkast (KN / M) | 7 | 7 | 7 |
8 | |
Flame-klasse |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 |
Test: A / B-ferhâlding is ferstelber, 130 ° C X 5MIN X 15MPA
Produktparameters | |||||
Produkt | GA-2041WY | GA-2051wY | GA-2061wy | GA-2071wY | |
Ferskining | Ljochtgriis | Ljochtgriis | Donker griis | Ljochtgriis | |
A / Bratio |
2: 100 | 2: 100 | 1: 1 | 2: 100 | |
Viscosity (PA.S) |
14-20 | 140-160 | 70-90 | 140-160 | |
Hurdens (Shorea) | 45 | 50 |
65 |
70 |
|
DENSITY (G / CM3) | 1.3 |
1.36 | 1.6 | 1.5 | |
Tensile krêft (MPA) | 2.5 |
3.0 |
3.0 |
3.0 |
|
ELONGATION (%) | 200 | 300 | 170 | 140 | |
Slachterkast (KN / M) | 7 | 7 | 7 |
8 | |
Flame-klasse |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 |