Ga-2041wy afo-retise ranon-tsolika misy ranon-tsolika ho an'ny coating (LSR)

Fampiharana: Mety amin'ny takelaka famokarana, takelaka fibre fitaratra, Coatingand Sponge Products. 
Endri-javatra fototra: Famatorana mafy miaraka amin'ny substrate, haingam-pandeha haingana haingana, tsara am-pitsarana tsara 「Amiceffect.
  • Ga-2041wy

  • Herchy

Fahafahana:
habe:

Fitsapana: A / B Ratio dia azo zahana, 130 ° C x 5min x 15mpa


Parameter vokatra
Vokatra Ga-2041wy Ga-2051wy Ga-2061w Ga-2071w
Bika Aman 'endrika Maimbo maivana Maimbo maivana Maizina volo Maimbo maivana
A / bratio
2: 100 2: 100 1: 1 2: 100
Viscosity (Pa.s)
14-20 140-160 70-90 140-160
Hardness (Shorea) 45 50
65
70
Fahalemena (G / CM3)

1.3

1.36 1.6 1.5
Hatanjoranana (MPA) 2.5
3.0
3.0
3.0
Elongation (%) 200 300 170 140
Hery mandatsa-dranomaso (kn / m) 7 7 7
8
Kilasy Flame
UL94V-0 UL94V-0 UL94V-0 UL94V-0









Teo aloha: 
Manaraka: 

Rohy haingana

Ny vokatra azontsika

ANTSIPIRIANY IFANDRAISANA

Manampy: Tsia .3, Lane 159, lalana Taiye, Distrika Fengxian, Shanghai
Tel / Whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Robber Co., Ltd. Sitemap |   Politika momba ny tsiambaratelo | Manohana avy amin'ny Leadong.