GA-2041WY
Herçi
| Elýeterliligi: | |
|---|---|
| mukdary: | |
Synag: A / B gatnaşygy sazlanýar, 130 ° C x 5min x 15MPa
| Önümiň parametrleri | |||||
| Haryt | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Daş görnüşi | Açyk çal | Açyk çal | Goňur çal | Açyk çal | |
| A / Bratio |
2: 100 | 2: 100 | 1: 1 | 2: 100 | |
| Iscapyşmazlyk (Pa.s) |
14-20 | 140-160 | 70-90 | 140-160 | |
| Gatylyk (ShoreA) | 45 | 50 |
65 |
70 |
|
| Dykyzlygy (g / cm3) | 1.3 |
1.36 | 1.6 | 1.5 | |
| Dartyş güýji (MPa) | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Uzalma (%) | 200 | 300 | 170 | 140 | |
| Göz ýaşyň güýji (kN / m) | 7 | 7 | 7 |
8 | |
| Ameangyn synpy |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |