Toets: A/B-verhouding is verstelbaar, 130°C x 5min x 15MPa
| Produk parameters | |||||
| Produk | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Voorkoms | Liggrys | Liggrys | Donkergrys | Liggrys | |
| A/Bratio |
2:100 | 2:100 | 1:1 | 2:100 | |
| Viskositeit (Pa.s) |
14-20 | 140-160 | 70-90 | 140-160 | |
| Hardheid (ShoreA) | 45 | 50 |
65 |
70 |
|
| Digtheid (g/cm3) | 1.3 |
1.36 | 1.6 | 1.5 | |
| Treksterkte (MPa) | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Verlenging (%) | 200 | 300 | 170 | 140 | |
| Skeursterkte (kN/m) | 7 | 7 | 7 |
8 | |
| Vlamklas |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |