GA-2041WY
Herchy
| Ku kumeka: | |
|---|---|
| Nhlayo: . | |
Xikambelo: A/B ratio ya lulamisiwa, 130°C x 5min x 15MPa
| Tipharamitha ta Xiendliwa . | |||||
| Ximakiwa | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Xivumbeko | Muhlovo wa grey wo vonikela | Muhlovo wa grey wo vonikela | Muhlovo wa wasi wo dzwihala | Muhlovo wa grey wo vonikela | |
| A/Bratio ya xirhendzevutani |
2:100 | 2:100 | 1:1 | 2:100 | |
| Viscosity(pa.s) . |
14-20 | 140-160 | 70-90 | 140-160 | |
| Ku nonon'hwa (Shorea) . | 45 | 50 |
65 |
70 |
|
| Ku tsindziyela(g/cm3) . | 1.3 |
1.36 | 1.6 | 1.5 | |
| Matimba ya ku tsana (MPA) . | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Ku leha(%) . | 200 | 300 | 170 | 140 | |
| Matimba ya ku handzuka (kN/m) . | 7 | 7 | 7 |
8 | |
| Tlilasi ya malangavi |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |