GA-2041WY
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
Muedzo: A/B reshiyo inochinjika, 130°C x 5min x 15MPa
| Product parameters | |||||
| Product | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Chitarisiko | Chiedza chepfumbu | Chiedza chepfumbu | Rima grey | Chiedza chepfumbu | |
| A/Bratio |
2:100 | 2:100 | 1:1 | 2:100 | |
| Viscosity(Pa.s) |
14-20 | 140-160 | 70-90 | 140-160 | |
| Kuoma (ShoreA) | 45 | 50 |
65 |
70 |
|
| Density(g/cm3) | 1.3 |
1.36 | 1.6 | 1.5 | |
| Tensile simba (MPa) | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Elongation(%) | 200 | 300 | 170 | 140 | |
| Simba rekubvarura (kN/m) | 7 | 7 | 7 |
8 | |
| Flame class |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |