GA-2041WY ƒe agbalẽ
Herchy ƒe ame
| Nusiwo Li: | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: A / B ƒe xexlẽme nye asitɔtrɔ, 130 ° C x 5min x 15MPa
| Nusiwo wowɔ ƒe nɔnɔmewo | |||||
| Nu si wowɔ | GA-2041WY ƒe agbalẽ | GA-2051WY ƒe agbalẽ | GA-2061WY ƒe agbalẽ | GA-2071WY ƒe agbalẽ | |
| Dzedzeme | Aŋutiɖiɖi si me kɔ | Aŋutiɖiɖi si me kɔ | Aŋutiɖiɖi viviti | Aŋutiɖiɖi si me kɔ | |
| A/Bratio ƒe xexlẽme |
2:100 me | 2:100 me | 1:1 | 2:100 me | |
| Viscosity(Pa.s) ƒe ʋeʋẽ lilili . |
14-20 me | 140-160 ƒe agbalẽa me | 70-90 me | 140-160 ƒe agbalẽa me | |
| Sesẽme (ƑutaA) . | 45 | 50 |
65 |
70 |
|
| Eƒe kpekpeme(g/cm3) . | 1.3 |
1.36 | 1.6 | 1.5 | |
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Elongation(%) ƒe didime . | 200 | 300 | 170 | 140 | |
| Aɖatsi ƒe ŋusẽ (kN/m) . | 7 | 7 | 7 |
8 | |
| Dzo ƒe klass |
UL94V-0 ƒe ƒuƒoƒo | UL94V-0 ƒe ƒuƒoƒo | UL94V-0 ƒe ƒuƒoƒo | UL94V-0 ƒe ƒuƒoƒo | |