GA-2041WY
Herchy
| Kasadiaan: | |
|---|---|
| Kuantitas: | |
Uji: Babandingan A/B tiasa disaluyukeun, 130°C x 5min x 15MPa
| Parameter produk | |||||
| produk | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Penampilan | kulawu caang | kulawu caang | kulawu poék | kulawu caang | |
| A/Bratio |
2:100 | 2:100 | 1:1 | 2:100 | |
| Viskositas (Pa.s) |
14-20 | 140-160 | 70-90 | 140-160 | |
| Teu karasa (ShoreA) | 45 | 50 |
65 |
70 |
|
| Kapadetan (g/cm3) | 1.3 |
1.36 | 1.6 | 1.5 | |
| Kakuatan tegangan (MPa) | 2.5 |
3.0 |
3.0 |
3.0 |
|
| Elongation(%) | 200 | 300 | 170 | 140 | |
| Kakuatan cimata (kN/m) | 7 | 7 | 7 |
8 | |
| Kelas seuneu |
UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |