GA-2040D Medium sareng High Voltage Insulated Liquid Silicone Rubber (LSR)

kasadiaan:
kuantitas:

Uji: Babandingan AB 1:1, 130°C x 5min x 15MPa

Parameter produk
produk GA-2040D
GA-2040D-45
GA-20400-60
Penampilan kulawu lampu / onta / beureum kulawu caang kulawu
ViskositasA (Pa·s)
250-400 70-100 1500-2000
ViskositasB (Pa·s)
250-400 70-100 1500-2000
Teu karasa (ShoreA) 43-48 37-43 55-60
Kapadetan (g/cm 3) 1.11
1.11
1.15
Kakuatan tegangan (MPa) 7
7.0
8.5
Elongation(%) 500 450 550
Kakuatan cimata (kN/m) 22
22
35
Konstanta diéléktrik dina 100HZ 3.03 2.95
3.3
Faktor dissipation at100HZ 0.0016 0.0017 0.004
Résistansi ka leakage listrik sareng nyirian 1A3.5 1A4.5 1A3.5
Kakuatan Diéléktrik (kV/mm) 24 .3
20.5
22
Volume Résistivitas (Ω·cm) 1.0 * 1015 1.0 * 1015 1.0 * 1015
Kelas seuneu FV-0 FV-0 FV-0





saméméhna: 
Teras: 

Tumbu Gancang

PRODUK KAMI

INPORMASI KONTAK

Tambahkeun: No.33, jalur 159, Taiye Jalan, Kacamatan Fengxian, Shanghai
Telepon / WhatsApp / Skype: +86 15221953351
Surélék:  info@herchyrubber.com
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Peta situs |   Kawijakan Privasi | Rojongan Ku Leadong.