GA-2040D Medium ma Voltage maualuga Insulated Suava Silicone Rubber (LSR)

Avanoa:
Tele:

Su'ega: AB ratio o le 1:1, 130°C x 5min x 15MPa

Fa'atauga o oloa
Oloa GA-2040D
GA-2040D-45
GA-20400-60
Fa'aaliga Efuefu mama/kamela/mumu Efuefu mumu Lanu efuefu
ViscosityA (Pa·s)
250-400 70-100 1500-2000
ViscosityB (Pa·s)
250-400 70-100 1500-2000
Malosi (ShoreA) 43-48 37-43 55-60
Malosi (g/cm 3) 1.11
1.11
1.15
Malosi fa'amalosi (MPa) 7
7.0
8.5
Fa'atele(%) 500 450 550
Malosi o loimata (kN/m) 22
22
35
Dielectric tumau i le 100HZ 3.03 2.95
3.3
Fa'aleaogaina ile 100HZ 0.0016 0.0017 0.004
Tete'e i le eletise eletise ma makaina 1A3.5 1A4.5 1A3.5
Malosi eletise (kV/mm) 24 .3
20.5
22
VolumeTa'ita'i (Ω·cm) 1.0 *1015 1.0 *1015 1.0 *1015
Vasega afi FV-0 FV-0 FV-0





Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.