Ọkara GA-2040D na nnukwu voltaji mkpuchi mmiri mmiri silicone rọba (LSR)

Nnweta:
Ọnụọgụ:

Nnwale: nha AB nke 1:1, 130°C x 5min x 15MPa

Ngwa ngwaahịa
Ngwaahịa GA-2040D
GA-2040D-45
GA-20400-60
Ọdịdị Agba ntụ ntụ/kamel/acha ọbara ọbara Agba ntụ dị nro Agba ntụ
ViscosityA (Pa·s)
250-400 70-100 1500-2000
ViscosityB (Pa·s)
250-400 70-100 1500-2000
Isi ike (ShoreA) 43-48 37-43 55-60
Njupụta(g/cm 3) 1.11
1.11
1.15
Ike tensile (MPa) 7
7.0
8.5
Mgbatị(%) 500 450 550
Ike akwa mmiri (kN/m) 22
22
35
Dielectric mgbe niile na 100HZ 3.03 2.95
3.3
Ihe nkwụsịtụ na 100HZ 0.0016 0.0017 0.004
Iguzogide ntapu eletrik na akara 1A3.5 1A4.5 1A3.5
Ike Dielectric (kV/mm) 24.3
20.5
22
Nkwụghachi olu (Ω·cm) 1.0 * 1015 1.0 * 1015 1.0 * 1015
Klas ire ọkụ FV-0 FV-0 FV-0





Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.