GA-2040D o'rta va yuqori kuchlanishli izolyatsiyalangan suyuq silikon kauchuk (LSR)

Mavjudligi:
Miqdori:

Sinov: AB nisbati 1:1, 130°C x 5min x 15MPa

Mahsulot parametrlari
Mahsulot GA-2040D
GA-2040D-45
GA-20400-60
Tashqi ko'rinish Och kulrang/tuya/qizil Och kulrang Kulrang
YopishqoqlikA (Pa·s)
250-400 70-100 1500-2000
YopishqoqlikB (Pa·s)
250-400 70-100 1500-2000
Qattiqlik (ShoreA) 43-48 37-43 55-60
Zichlik (g/sm 3) 1.11
1.11
1.15
Kuchlanish kuchi (MPa) 7
7.0
8.5
Uzayish (%) 500 450 550
Yirilish kuchi (kN/m) 22
22
35
100 Gts da dielektrik doimiy 3.03 2.95
3.3
100 Gts da tarqalish koeffitsienti 0.0016 0.0017 0.004
Elektr qochqinning qarshiligi va markalash 1A3.5 1A4.5 1A3.5
Dielektrik quvvat (kV/mm) 24 .3
20.5
22
Ovoz qarshiligi (Ō·sm) 1,0 *1015 1,0 *1015 1,0 *1015
Olovli sinf FV-0 FV-0 FV-0





Oldingi: 
Keyingisi: 

TEZKOR havolalar

MAHSULOTLARIMIZ

BOG'LANISH UCHUN MA'LUMOT

Qo'shish: №33, 159-ko'cha, Taiye yo'li, Fengxian tumani, Shanxay
Tel / WhatsApp / Skype: +86 15221953351
Mualliflik huquqi     2023 Shanghai Herchy Rubber Co., Ltd. Sayt xaritasi |   Maxfiylik siyosati | Qo'llab-quvvatlash Leadong.