Gwaji: rabon AB na 1:1, 130°C x 5min x 15MPa
| Siffofin samfur |
|
| Samfura |
GA-2040D
|
GA-2040D-45
|
GA-20400-60
|
| Bayyanar |
Haske mai launin toka/rakumi/ja |
Launi mai launin toka |
Grey |
ViscosityA (Pa·s)
|
250-400 |
70-100 |
1500-2000
|
ViscosityB (Pa·s)
|
250-400 |
70-100 |
1500-2000 |
| Hardness (ShoreA) |
43-48 |
37-43 |
55-60 |
| Girma (g/cm 3) |
1.11
|
1.11
|
1.15
|
| Ƙarfin ɗaure (MPa) |
7
|
7.0
|
8.5
|
| Tsawaita(%) |
500 |
450 |
550 |
| Ƙarfin hawaye (kN/m) |
22
|
22
|
35
|
| Dielectric akai-akai a 100HZ |
3.03 |
2.95
|
3.3 |
| Matsakaicin ɓarna a 100HZ |
0.0016 |
0.0017 |
0.004 |
| Juriya ga zubewar lantarki da yin alama |
1A3.5 |
1A4.5 |
1A3.5 |
| Ƙarfin Dielectric (kV/mm) |
24.3
|
20.5
|
22
|
| Resistivity (Ω·cm) |
1.0 * 1015 |
1.0 * 1015 |
1.0 * 1015 |
| Ajin harshen wuta |
FV-0 |
FV-0 |
FV-0 |