Jaribio: uwiano wa AB wa 1 :1, 130°C x 5min x 15MPa
| Vigezo vya bidhaa |
|
| Bidhaa |
GA-2040D
|
GA-2040D-45
|
GA-20400-60
|
| Muonekano |
Kijivu hafifu/ngamia/nyekundu |
Kijivu nyepesi |
Kijivu |
MnatoA (Pa·s)
|
250-400 |
70-100 |
1500-2000
|
MnatoB (Pa·s)
|
250-400 |
70-100 |
1500-2000 |
| Ugumu (ShoreA) |
43-48 |
37-43 |
55-60 |
| Uzito (g/cm 3) |
1.11
|
1.11
|
1.15
|
| Nguvu ya mkazo (MPa) |
7
|
7.0
|
8.5
|
| Kurefusha(%) |
500 |
450 |
550 |
| Nguvu ya machozi (kN/m) |
22
|
22
|
35
|
| Dielectric mara kwa mara katika 100HZ |
3.03 |
2.95
|
3.3 |
| Kipengele cha kutoweka katika 100HZ |
0.0016 |
0.0017 |
0.004 |
| Upinzani wa kuvuja kwa umeme na kuashiria |
1A3.5 |
1A4.5 |
1A3.5 |
| Nguvu ya Dielectric (kV/mm) |
24 .3
|
20.5
|
22
|
| Usaidizi wa Kiasi (Ω·cm) |
1.0 *1015 |
1.0 *1015 |
1.0 *1015 |
| Darasa la moto |
FV-0 |
FV-0 |
FV-0 |