Ka ethylene, propylene le non-conjugated diolefin copolymerization ea ethylene propylene diene rabara (EPDM) kaha lisebelisoa tsa terata le lisebelisoa tsa cable li na le lilemo tse fetang 60 tsa histori. EPDM le polyvinyl chloride (PVC) le cross-linked polyethylene (XLPE) le lisebelisoa tse ling tse sireletsang li na le boemo bo tšoanang bo ke keng ba e-ba teng, 'me melemo ea eona e ikhethang ke: bophelo bo bolelele ba tšebeletso, ho hanyetsa metsi le oksijene le botsitso ba mocheso, mefuta e mengata e pharaletseng ea mocheso o sebetsang. Ha ts'ebeliso ea EPDM tšimong ea ho kenya motlakase e ntse e pharalla le ho feta, litlhoko tsa matšoao a bohlokoa a EPDM le tsona li batla li le boima le ho feta, haholo-holo lits'ebetsong tse ling tsa maemo a holimo, taolo ea matšoao a mantlha a EPDM e na le litlhoko tse thata, ha feela matšoao a bohlokoa a lumellanang a le maemong a lekaneng, e le hore EPDM e finyelle ts'ebetso, ts'ebetso le ts'ebeliso ea litlhoko. Nka EPDM e le mohlala bakeng sa ho etsa terata e mahareng-voltage le thapo e sireletsang kabel, haeba matla tensile, tabola elongation, matla senya, dielectric tahlehelo, bophahamo ba modumo resistivity le tse ling tse bohlokoa mechine le thepa ea motlakase ea sehlahisoa ka kopana le ditlhoko, thepa e tala EPDM ethylene content, mooney viscosity, dikahare diolefin le bohloeki le matšoao a mang a bohlokoa a lokela ho ba le meeli ea bohlokoa. Ho na le lintlha tse ngata tse amang khanyetso ea ho senyeha ha terata ea EPDM le insulation ea cable. Ntle le litaba tse boletsoeng ka holimo tsa ethylene, dikahare tsa diolefin le bohloeki, li-gel content ho EPDM, hammoho le ho lokisoa le ho ntlafatsa mokhoa oa ho sebetsa li na le phello ea bohlokoa ho hanyetsa ho senyeha ha sehlahisoa. Hase feela lintlha tse susumetsang tse le 'ngoe le tse ka thōko, empa hape li sebetsa hammoho ho ba le phello e pharaletseng ea ho hanyetsa motlakase oa lihlahisoa. Leqepheng lena, lintlha tse ling tse amang ho hanyetsa ho senyeha ha EPDM li khethiloe bakeng sa lipatlisiso le tlhahlobo e hlophisitsoeng, e le ho fana ka boitsebiso ba bohlokoa bakeng sa ho qaptjoa ha lihlahisoa tsa EPDM bakeng sa terata le lisebelisoa tsa cable.
1 Phello ea litaba tsa ENB ho matla a ho senya
Likahare tsa ENB (karolo ea boima) <4.5%, 'me ka keketseho ea litaba tsa ENB, matla a ho senya sehlahisoa a fokotseha; Likahare tsa ENB (karolo ea boima) ≥4.5%, 'me ka keketseho ea litaba tsa ENB (karolo ea bongata), matla a ho senya sehlahisoa a eketseha.
2. Tšusumetso ea bohloeki ba rabara ho matla a ho senya
Ha EPDM e sebelisoa ts'ebetsong ea lisebelisoa tsa motlakase tsa motlakase, ho hloeka ha thepa ho hlokahala ho isa tekanyong e itseng. Ho hloeka ha EPDM hangata ho hlalosoa ka mokhoa oa molora, oo haholo-holo o entsoeng ka letsoai le sa tloaelehang le nang le li-ion tsa tšepe (vanadium, aluminium, tšepe, sodium, joalo-joalo) tse hlahisoang nakong ea polymerization le post-processing, hammoho le litšila tse tsoang linaheng tse ling. Ho ba teng ha molora, ho lekanang le 'sekoli' sa 'mele, habonolo ho fetoha katleho ea lihlahisoa tsa rabara ka ho tsosoa ke motlakase. Ha lihlahisoa tsa molora ho EPDM li ntse li eketseha, li-ion tsa tšepe tsa sampuli li boetse lia eketseha, 'me matla a ho senya sehlahisoa se felile a fokotseha. Molora (li-ion tsa tšepe, litšila tse tsoang kantle ho naha) o na le phello e itseng ts'ebetsong ea ho senyeha ha motlakase ea sehlahisoa. Ha ho nahanoa ka phello ea li-ion tsa tšepe ho hanyetsa ho senyeha ha sehlahisoa, li-ion tsa tšepe tsa sampole ea teko li tla theha sebaka sa sebaka ka hare ho sehlahisoa tlas'a ts'ebetso ea sebaka sa motlakase se ka ntle, se tla be se le holimo le tšimo e ka ntle ho senya sehlahisoa. Ha litaba tsa li-ion tsa tšepe tsa sampole li ntse li eketseha, matla a masimong a ka hare a ntse a eketseha butle-butle, 'me monyetla oa ho bokellana ha li-ion tsa tšepe o ntse o eketseha, ho fella ka matla a sebaka se phahameng ka mokhoa o sa tloaelehang,' me lintlha tsena kaofela li tla fokotsa ho hanyetsa ho senyeha ha sehlahisoa. Ea bobeli, nahana ka phello ea litšila tse tsoang linaheng tse ling ho hanyetsa ho senyeha ha lihlahisoa, lihlahisoa tsa rabara ka litšila tse tsoang linaheng tse ling haholo-holo li kenyelletsa lehlabathe le mafome, joalo-joalo, hangata, litšila tsena le lihlahisoa tsa rabara li lumellana haholo, 'me boteng ba tsona bakeng sa lihlahisoa tsa rabara bo lekana le 'sekoli', se senya ho tšoana le botšepehi ba lihlahisoa tsa rabara. Ha tšimo ea motlakase e tsoang ka ntle e sebetsa ho lihlahisoa tsa motlakase tsa EPDM tse nang le 'mefokolo', ho tla ba bonolo ho phunyeletsa lihlahisoa tsa motlakase ho 'mefokolo', kahoo ho fokotsa ho hanyetsa ha sehlahisoa ho senya motlakase.
3. Tšusumetso ea litaba tsa gel ho matla a ho senya
Gel ke mohaho o khethehileng oa 'likaroloana tsa rabara' tse entsoeng nakong ea polymerization ea EPDM. Ka lebaka la morphology ea eona e khethehileng le sebopeho, tšebelisano ea eona le ketane e tloaelehileng ea molek'hule sehlahisoa sa rabara e batla e fokola, 'me boteng ba eona bo ka boela ba nkoa e le 'ho se hloeke' ho setseng sehlahisoa sa rabara. '. Bakeng sa lihlahisoa tsa boleng bo phahameng ba EPDM tsa motlakase oa motlakase, lihlahisoa tsa gel li ka boela tsa e-ba le tšusumetso mosebetsing oa ho senyeha ha motlakase oa sehlahisoa. Ha lihlahisoa tsa gel ho EPDM li ntse li eketseha, matla a ho senya sehlahisoa se felile a fokotseha. Kaha gel ke sebopeho sa marang-rang a marang-rang, morphology ea eona e fapane haholo le ea liketane tse tloaelehileng tsa EPDM tsa molek'hule, 'me ka hona ha e lumellane le limolek'hule tsa DMDM tse tloaelehileng ho feta limolek'hule tsa DMDM le lik'hemik'hale tsa EPDM. bokaholimo ba gel le liketane tse tloaelehileng tsa limolek'hule li fokola ho feta tse pakeng tsa liketane tse tloaelehileng tsa EPDM Matla a ho sebelisana pakeng tsa bokaholimo ba gel le liketane tse tloaelehileng tsa limolek'hule li fokola ho feta pakeng tsa liketane tse tloaelehileng tsa EPDM, 'me bokaholimo ba gel ha bo hlile ha bo 'tlale' ka liketane tsa EPDM.
Bokaholimo ba gel ha bo hlile ha bo 'tlale' ka liketane tsa limolek'hule tsa EPDM, 'me ho ka ba le 'likheo' tse ling. Kaha ho ba teng ha gel ho tla ama homogeneity ea sehlahisoa, sehlahisoa se sebelitsoeng se tla etsa sekhahla sa tšimo se pota-potileng gel tlas'a ts'ebetso ea matla a ka ntle a matla a motlakase. Phapang e kholoanyane pakeng tsa morphology le sebopeho sa gel le liketane tsa limolek'hule tsa EPDM tse potolohileng, ho thehoa ho hoholo ha sekhahla sa tšimo, ho bonolo ho senya bokaholimo ba gel e nang le matla a lekanyelitsoeng a fokolang 'me ho ka ba le 'lekhalo' sehlahisoa. Ha ho ntse ho e-na le phapang pakeng tsa liketane tsa limolek'hule tsa EPDM, ho na le sekhahla se seholo sa tšimo, ho na le monyetla o moholo oa ho senya bokaholimo ba gel moo matla a lekanyelitsoeng a fokolang 'me ho ka ba le 'likheo', ho theha 'mefokolo' sehlahisoa, se lebisang ho senyeha ha sampuli pele, 'me kahoo ho fokotsa ts'ebetso ea ho senyeha ha sampuli.
4. Tšusumetso ea mokhoa oa ho sebetsa ho matla a ho senya
Foromo ea ts'ebetso ke sehokelo sa bohlokoa ts'ebetsong ea lihlahisoa tsa EPDM ho lihlahisoa tsa motlakase oa motlakase, empa hape le e 'ngoe ea lintlha tsa bohlokoa tse amang ts'ebetso ea ho senyeha ha lihlahisoa tsa motlakase. Litokiso le ntlafatso ea mokhoa oa mantlha oa ts'ebetso le ho eketsoa ha li-additives tsa motlakase li ka ntlafatsa haholo ts'ebetso ea ho senyeha ha lihlahisoa tsa motlakase. Ka mor'a hore lisebelisoa tse tala tsa EPDM li sebetsanoe ho latela mekhoa e fapaneng, thepa ea mechine ha e fetohe haholo, 'me ea morao-rao e ka ba 5% feela e phahameng ho feta ea pele, empa matla a ho senya motlakase a na le phetoho e kholo,' me ea morao-rao e ka bang 60% e phahameng ho feta ea pele. Lebaka le ka sehloohong la ntlafatso ea thepa ea mechine le ea motlakase ke hore moetsi oa lithapo tsa leoatleng o ntlafalitse tekanyo ea diisopropyl benzene peroxide nakong ea ts'ebetso ea lihlahisoa, e le hore litlamo tse peli tse lehlakoreng la ENB li kopane ka ho feletseng, 'me li-bond tse setseng tse peli li fokotsehe,' me kaolin le lisebelisoa tse ling tsa motlakase li kenngoa, tse eketsang ts'ebetso le ts'ebetso e setseng. lihlahisoa. Lintlha tse peli tse ka holimo li lekane ho paka bohlokoa ba mokhoa oa ho sebetsa ho ntlafatsa ts'ebetso ea ho senya motlakase oa lihlahisoa tsa motlakase tsa EPDM.
5.Qetello
(1) Tlamo e habeli ka lehlakoreng la ketane ea monoma ea boraro (ENB) ho EPDM e hokahane ka ho lekaneng.
(1) EPDM ka monoma ea boraro (ENB) ka lehlakoreng la ketane ea tlamahano e 'meli, ha e ntse e hokahane ka ho feletseng, e fokotsa palo ea masala, e leng e loketseng haholoanyane ho lihlahisoa tsa motlakase oa motlakase (terata le lisebelisoa tsa cable) ts'ebetso ea ho hanyetsa ho senyeha ha motlakase.
(2) Ho hloeka ha thepa e tala ea EPDM e phahameng (e theohile ka tlaase ho molora), ho thusa haholo bakeng sa ntlafatso ea lihlahisoa tsa motlakase oa motlakase (terata le lera la ho kenya lisebelisoa) ho hanyetsa ho senyeha ha motlakase.
(3) Ho theola li-gel content tsa EPDM lihlahisoa tse tala, ho thusa ho ntlafatsa lihlahisoa tsa motlakase tsa motlakase (wire le cable insulation) ho hanyetsa ho senyeha ha motlakase.
(3) Ho theola li-gel tsa lihlahisoa tse tala tsa EPDM, ho molemo ho hanyetsa ho senyeha ha lihlahisoa tsa motlakase oa motlakase (terata le lisebelisoa tsa cable).
(4) Ho fetola palo ea EPDM ka mokhoa oa motheo oa li-insulators tsa motlakase (terata le lisebelisoa tsa motlakase) le ho e tlatsa ka lisebelisoa tsa motlakase tsa motlakase ho ka ntlafatsa haholo ho hanyetsa ho senyeha ha li-insulators tsa motlakase (terata le lisebelisoa tsa motlakase).