Kei konei koe: Kainga » Rongorongo » Rongorongo » Ko nga mea e pa ana ki te pakaru o te waea rapa ethylene propylene me te paparanga arai taura.

Ko nga mea e pa ana ki te pakaru o te waea rapa ethylene propylene me te paparanga arai taura

Tirohanga: 0     Kaituhi: Kaiwhakatika Pae Wā Whakaputa: 2023-08-13 Takenga: Pae

Uiui

Na te ethylene, propylene me te kore-conjugated diolefin copolymerization o te ethylene propylene diene rapa (EPDM) hei waea me te taura taura kua neke atu i te 60 tau o te hitori. Ko te EPDM me te polyvinyl chloride (PVC) me te polyethylene hono-whiti (XLPE) me etahi atu mea whakamarumaru he rite tonu te tuunga e kore e taea te whakakapi, me ona painga ahurei ko: te roa o te ratonga, he pai ake te aukati ki te wai me te hāora me te pumau o te waiariki, te whanuitanga o te pāmahana whakahaere. I te mea ko te tono o te EPDM i roto i te mara o te whakamaarama hiko he nui ake te whanui, ko nga whakaritenga o nga tohu matua EPDM he nui ake te tono, ina koa i etahi tono teitei, ko te mana o nga tohu matua o te EPDM he nui ake nga whakaritenga, ko nga tohu matua e rite ana kei roto i te awhe whaitake, kia tutuki ai te EPDM ki te tukatuka, ki te mahi me te whakamahi i nga whakaritenga. Tangohia te EPDM hei tauira mo te hanga o te waea reo-ngaohiko me te whakamaarama taura, mena ko te kaha o te kaha, te haehae elongation, te kaha pakaru, te mate dielectric, te aukati rōrahi me etahi atu taonga miihini me te hiko o te hua ka taea te whakatutuki i nga whakaritenga, ko te rauemi mata EPDM ethylene ihirangi, mooney viscosity, te ihirangi diolefin me te ma me etahi atu tohu tohu matua. He maha nga mea e pa ana ki te aukati pakaru o te waea EPDM me te tauera taura. I tua atu i te ihirangi ethylene kua whakahuahia i runga ake nei, te ihirangi diolefin me te parakore, te ihirangi gel i roto i te EPDM, tae atu ki te whakatikatika me te arotautanga o te tikanga tukatuka he paanga nui ki te aukati pakaru o te hua. Ehara i te mea ko nga mea whakaawe takitahi me te taratahi, engari ka mahi tahi ano kia whai paanga matawhānui ki te aukati hiko o nga hua. I roto i tenei pepa, ko etahi o nga mea e pa ana ki te aukati pakaru o te EPDM ka tohua mo te rangahau nahanaha me te tātari, hei whakarato tohutoro nui mo te whakahiatotanga o nga hua EPDM mo te waea me te taura taura.


1 Te paanga o te ihirangi ENB mo te kaha pakaru


Ko te ihirangi ENB (hautanga papatipu) <4.5%, me te piki ake o te ihirangi ENB, ka heke te kaha pakaru o te hua; Ko te ihirangi ENB (hautanga papatipu) ≥4.5%, me te piki ake o te ihirangi ENB (hautanga papatipu), ka piki ake te kaha pakaru o te hua.


2. Te awe o te rapa parakore ki te kaha pakaru


I te wa e whakamahia ana te EPDM i roto i te tukatuka o nga taputapu hiko hiko, ka hiahiatia te ma o te rauemi ki tetahi waahanga. Ko te ma o te EPDM te nuinga o te wa e whakaatuhia ana i roto i nga waahanga o te pungarehu, ko te nuinga o nga tote parakore kei roto i nga katote whakarewa (vanadium, konumohe, rino, konutai, me etahi atu) i whakauruhia i te wa o te polymerization me te tukatuka i muri mai, me nga poke ke. Ko te noho o te pungarehu, he rite ki te 'koha' tinana, ka ngawari te pakaru i roto i nga hua rapa na te wiri hiko. I te piki ake o te pungarehu i roto i te EPDM, ka piki ake te ihirangi katote whakarewa i roto i te tauira, ka heke te kaha pakaru o te hua kua oti. Ko te pungarehu (katote konganuku, ko nga poke ke) ka pa ki te mahi pakaru hiko o te hua. Ma te whakaaro ki te paanga o nga katote whakarewa i runga i te aukati pakaru o te hua, ko nga katote whakarewa i roto i te tauira whakamatautau ka hanga he mara rohe i roto i te hua i raro i te mahi a te papa hiko o waho, ka whakakikoruatia ki te mara o waho ki te kino i te hua. Ka piki ake te ihirangi o nga katote whakarewa i roto i te tauira, ka piki haere te kaha o te mara o roto, me te kaha o te whakahiato o nga katote whakarewa i te rohe, ka hua mai i nga kaha o te waahi o te rohe, a ko enei mea katoa ka whakaiti i te aukati pakaru o te hua. Tuarua, whakaarohia te paanga o nga poke o kee ki te pakaru o nga hua, nga hua rapa i roto i nga poke o waho ko te nuinga o te kirikiri me te waikura, me era atu, ko enei poke me nga hua rapa he tino ngoikore te hototahitanga, a ko to ratou aroaro mo nga hua rapa he rite ki te 'koha', ka whakangaro i te rite me te pono o nga hua rapa. I te wa e mahi ana tetahi mara hiko ngaohiko teitei o waho i runga i nga hua whakahiato hiko EPDM me nga 'koha', ka ngawari te pakaru i roto i nga hua whakamaarama hiko i nga ' koha ', na reira ka whakaiti i te aukati o te hua ki te pakaru hiko.


3. Te awe o te ihirangi gel ki te kaha pakaru


Ko te kaera he hanganga motuhake o 'matūriki rapa' i hangaia i te wa o te polymerization o EPDM. Na tona ahua motuhake me tona hanganga, he ngoikore te hononga ki te mekameka ngota noa i roto i te hua rapa, ka taea hoki te kii he 'para' kei roto i te hua rapa. '. Mo nga hua whakahiato hiko EPDM kounga teitei, ka whai paanga ano te ihirangi rei ki te mahi pakaru hiko o te hua. I te pikinga o te reera kei roto i te EPDM, ka heke te kaha pakaru o te hua kua oti. I te mea he hanganga mata hono te gel, he rereke te ahua o te ahua o te momo o te EPDM noa o nga mekameka ngota ngota EPDM, na reira he iti ake te hototahi ki te mekameka EPDM me te mekameka rapoi EPDM. he ngoikore ake te pahekoheko i waenga i te mata rii me nga mekameka ngota ngota noa i tera i waenga i nga mekameka ngota ngota EPDM noa Ko te kaha tauwhitinga i waenga i te mata rii me nga mekameka ngota noa he ngoikore ake i tera i waenga i nga mekameka ngota ngota EPDM noa, a ko te mata o te reera karekau i te 'whakakii' ki nga mekameka ngota ngota EPDM.


Ko te mata o te reera kaore i te mea 'whakakii' ki nga mekameka ngota ngota EPDM, a tera pea he 'aputa'. I te mea ko te noho o te ra ka pa ki te riterite o te hua, ka hangaia e te hua tukatuka he rōnaki mara huri noa i te kiri i raro i te mahi a te papa hiko hiko teitei o waho. Ko te nui ake o te rereketanga i waenga i te ahua me te hanganga o te kaera me nga mekameka ngota ngota EPDM a tawhio noa, ka nui ake te hanga o te rōnaki mara, ka ngawari ake te pakaru i te mata o te reera he ngoikore ake te kaha o te whanaungatanga, a he 'gap' kei roto i te hua. Ko te nui ake o te rereketanga i waenga i nga mekameka ngota ngota EPDM, ka nui ake te rōnaki mara, ka kaha ake te whakangaro i te mata o te kiri kei te ngoikore te kaha o te whanaungatanga, a tera pea he 'aputa', ka puta he 'koha' i roto i te hua, e arai ana ki te pakaru wawe o te tauira, me te whakaiti i te mahi pakaru o te tauira.


4. Te awe o te tikanga tukatuka ki te kaha pakaru


Ko te tikanga tukatuka he hononga matua ki te tukatuka o nga hua EPDM ki nga hua whakaahuru hiko, engari ko tetahi o nga mea matua e pa ana ki te pakaru o nga hua o te hiko. Ko te whakatikatika me te arotautanga o te tikanga tukatuka taketake me te taapiri o nga taapiri whakamaarama hiko ka taea te whakapai ake i nga mahi pakaru o nga hua whakamaarama hiko. I muri i te tukatuka o taua rauemi mata EPDM kia rite ki nga tauira rereke, kaore e nui te whakarereketanga o nga taonga miihini, a ko te mea whakamutunga ko te 5% teitei ake i te waa o mua, engari ko te kaha o te pakaru o te hiko he huringa nui, a ko te mea whakamutunga ko te 60% teitei ake i te waa o mua. Ko te take nui mo te whakapai ake i nga taonga miihini me te hiko na te kaihanga taura moana kua pai ake te inenga o te diisopropyl benzene peroxide i te wa e tukatuka ana nga hua, kia honoa ai nga hononga takirua o te mekameka taha o te ENB, a ka whakahekehia nga toenga o nga here rua, ka taapirihia te kaolin me etahi atu taapiri hiko, e mau tonu ana te mahi, me te whakatairanga i nga hua. Ko nga tohu e rua i runga ake nei e ranea ana hei whakamatau i te hiranga o te tikanga tukatuka hei whakapai ake i te mahi pakaru o te hiko o nga hua whakawera hiko EPDM.


5.Whakamutunga

(1) Ko te hononga takirua i roto i te mekameka taha o te monomer tuatoru (ENB) i roto i te EPDM he pai ake te hono-whakawhiti.

(1) EPDM i roto i te tuatoru monomer (ENB) i roto i te mekameka taha o te here rua, te atu tino whiti-hononga, te iti te maha o toenga, te pai ake ki te hua te hiko (waea me te taura insulation) mahi ātete pakaruhanga hiko.

(2) Ko te teitei ake o te parakore o te EPDM raw rauemi (ko te iti iho o te ihirangi pungarehu), ka nui ake te awhina mo te whakapai ake i nga hua hiko hiko (waea me te paparanga taura) te aukati hiko.

(3) Ko te iti ake o te reera o nga rauemi mata EPDM, ka nui ake te awhina ki te whakapai ake i nga hua whakamaarama hiko (waea me te taura taura) te aukati pakaru hiko.

(3) Ko te iti ake o te kiko o te reera o te rauemi mata EPDM, ka pai ake te aukati i te pakaru o nga hua whakamaarama hiko (waea me te taura taura).

(4) Ko te whakatikatika i te nui o te EPDM i roto i te hanga turanga o nga kaitarai hiko (waea me te taura taura) me te taapiri atu ki nga taapiri whakauru hiko ka taea te whakapai ake i te aukati pakaru o nga kaitarai hiko (waea me te taura taura).


NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Takiwa Fengxian, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.