uripano Kumba » News News Iwe :

Zvinhu zvinokanganisa kuparara kwekupokana kwe ethylene propylene rubber waya uye tambo yekumisa tambo

Maonero: 0     Munyori: Saiti Edhita Nguva Yekuburitsa: 2023-08-13 Mabviro: Site

Bvunza

Ne ethylene, propylene uye isina-conjugated diolefin copolymerization ye ethylene propylene diene rubber (EPDM) sewaya uye tambo yekuvharisa zvinhu zvine makore anopfuura makumi matanhatu enhoroondo. EPDM uye polyvinyl chloride (PVC) uye muchinjika-yakabatana polyethylene (XLPE) uye zvimwe insulating zvinhu vane zvakafanana irreplaceable nzvimbo, uye zvakanakira ayo akasiyana siyana ndeiyi: refu upenyu basa, nani kuramba mvura uye okisijeni uye kupisa kugadzikana, yakafara siyana kushanda tembiricha. Sezvo kushandiswa kweEPDM mumunda wekudzivirira kwemagetsi kunowedzera kuwedzera, zvinodiwa zveEPDM zvakakosha zviratidzo zvinowedzerawo uye zvakanyanya kudiwa, kunyanya mune mamwe maitiro ekupedzisira, kutonga kwezviratidzo zvakakosha zveEPDM kune zvakanyanya kuoma zvinodiwa, chete kana zviratidzo zvakakosha zvinowirirana zviri muhutano hunonzwisisika, kuitira kuti EPDM isangane nekugadzirisa, kushanda uye kushandiswa kwezvinodiwa. Tora EPDM semuenzaniso wekugadzirwa kwepakati-voltage waya uye tambo yekuvharisa, kana simba rekusimba, kubvarura kurebesa, kuparara kwesimba, dielectric kurasikirwa, vhoriyamu resistivity uye zvimwe zvakakosha zvemagetsi uye zvemagetsi zvechigadzirwa zvinogona kusangana nezvinodiwa, iyo mbishi zvinhu EPDM ethylene content, mooney viscosity, diolefin zvemukati uye kuchena uye zvimwe zvinogumira zviratidzo zvinokosha zvinofanira kuva nemiganhu inokosha. Pane zvinhu zvakawanda zvinokanganisa kuparara kwekupokana kweEPDM waya uye tambo yekuvharisa. Pamusoro peiyo yakataurwa pamusoro ethylene yemukati, diolefin yemukati uye kuchena, iyo gel yemukati muEPDM, pamwe nekugadzirisa uye optimization yefomati yekugadzira ine kukosha kwakakosha pakuramba kuparara kwechigadzirwa. Havasi ivo chete uye vari voga vanopesvedzera zvinhu, asi zvakare vanoshanda pamwe chete kuti ive nemhedzisiro yakazara pakupokana kwemagetsi kushorwa kwezvigadzirwa. Mune pepa iri, zvimwe zvezvinhu zvinokanganisa kushorwa kweEPDM zvinosarudzwa kuti zviongorore uye zviongorore, kuitira kuti zvipe zvakakosha zvinyorwa zvekugadzirwa kweEPDM kune tambo uye tambo.


1 Mhedzisiro yeENB yezvinyorwa pane kuparara kwesimba


ENB zvinyorwa (chikamu chemazana) <4.5%, uye nekuwedzera kweENB zvinyorwa, simba rekuparara kwechigadzirwa rinoderera; ENB yemukati (chikamu chechikamu) ≥4.5%, uye nekuwedzera kweENB yemukati (chikamu chezhinji), kuparara kwesimba kwechigadzirwa kunowedzera.


2. Pesvedzero yekuchena kwerabha pane kuparara kwesimba


Kana EPDM inoshandiswa mukugadzirisa magetsi ekudzivirira zvinhu, kuchena kwezvinhu kunodiwa kune imwe nhanho. Kuchena kweEPDM kunowanzo kuratidzwa maererano neash content, iyo inonyanya kuumbwa neinorganic salts ine metal ions (vanadium, aluminium, iron, sodium, etc.) inounzwa panguva yepolymerization uye post-processing, pamwe chete nekusvibiswa kune dzimwe nyika. Kuvapo kwedota, yakaenzana ne 'chirema' chemuviri, chinova nyore kuburitsa muzvigadzirwa zverabha nekuvhunduka kwemagetsi. Sezvo madota ari mu EPDM anowedzera, iyo ion yesimbi mumuenzaniso inowedzerawo, uye kuparara kwesimba kwechigadzirwa chakapedzwa kunoderera. Madota (metal ions, tsvina yekunze) ine imwe mhedzisiro pakuparara kwemagetsi kwechigadzirwa. Tichifunga nezve mhedzisiro yeioni yesimbi pakuputsika kwechigadzirwa, iyo simbi yesimbi muyedzo sampu inoumba nzvimbo yenzvimbo mukati mechigadzirwa pasi pechiito chekunze kwemagetsi emagetsi, ayo anozove akakwiridzirwa nemunda wekunze kukuvadza chigadzirwa. Sezvo zviri mukati mesimbi ions mumuenzaniso zvichiwedzera, simba remukati remunda rinowedzera zvishoma nezvishoma, uye mukana wekubatanidzwa kweayoni yesimbi inowedzerawo, zvichikonzera kusimba kwakanyanya kwenzvimbo, uye izvi zvese zvinoderedza kuparara kwechigadzirwa. Chechipiri, funga nezvekukanganisa kwekune dzimwe nyika pakuputsika kwezvigadzirwa, zvigadzirwa zverabha mune kusvibiswa kwekunze kunyanya zvinosanganisira jecha uye ngura, nezvimwewo, kazhinji, izvi zvinosvibisa uye zvigadzirwa zverabha hazvienderane zvakanaka, uye kuvapo kwavo kune zvigadzirwa zverabha zvakaenzana ne 'kukanganisa', zvichiparadza kufanana uye kutendeseka kwezvigadzirwa zverabha. Kana yekunze high-voltage yemagetsi munda inobata EPDM magetsi ekudzivirira zvigadzirwa ne 'defects', zvichava nyore kupaza nepakati pemagetsi ekudzivirira zvigadzirwa pa 'defects', nokudaro kuderedza chigadzirwa kuramba kuparara kwemagetsi.


3. Pesvedzero yezvinyorwa zvegel pane simba rekuputsika


Gel chimiro chakakosha che 'rubber particles' chakaumbwa panguva yepolymerization yeEPDM. Nekuda kwechimiro chayo chakakosha uye chimiro, kudyidzana kwayo neyakajairwa molecular cheni muchigadzirwa cherabha haina kusimba, uye kuvepo kwayo kunogonawo kutorwa se 'kusachena' kwasara muchigadzirwa cherabha. '. Pamusoro pezvigadzirwa zvemhando yepamusoro zveEPDM zvemagetsi zvekudzivirira, gel yemukati inogonawo kukanganisa kuparara kwemagetsi echigadzirwa. Sezvo iyo gel yemukati muEPDM ichiwedzera, kuparara kwesimba rechigadzirwa chakapedzwa kunoderera. Sezvo gel iri crosslinked mesh chimiro, morphology yayo yakasiyana zvakanyanya neyeyakajairwa EPDM molecular cheni, uye saka haina kuenderana neakajairika ma molecular, DMDM chains pakati pemamolecular chains EP. iyo gel yepamusoro uye yakajairwa mashetani emaketani haina kusimba kupfuura iyo pakati peyakajairwa EPDM mashetani emaketani Isimba rekubatana pakati peiyo gel kumusoro uye yakajairika mashetani eketani haina kusimba kupfuura iyo iri pakati peyakajairika EPDM maketani emaketani, uye iyo gel yepamusoro haireve 'yakazadzwa' neEPDM mashetani emaketani.


Kumusoro kwejeri hakurevi 'kuzadzwa' neEPDM molecular cheni, uye panogona kunge paine 'magapu'. Sezvo kuvapo kwejeri kuchakanganisa homogeneity yechigadzirwa, chigadzirwa chakagadziridzwa chichagadzira munda wakakomberedza gel pasi pekuita kwekunze kwepamusoro-voltage yemagetsi. Iyo misiyano yakakura pakati pe morphology uye chimiro chejeri uye yakapoteredza EPDM molecular maketani, iyo yakakura kuumbwa kwemunda gradient, zviri nyore kuputsa pamusoro pejeri rine simba risina simba uye panogona kuva ne 'gap' muchigadzirwa. Kunyanya mutsauko pakati peEPDM molecular chain, iyo yakakura gradient yemunda, zvakanyanya kuparadza gel pamusoro apo simba rehukama harina simba uye panogona kunge paine 'magapu', achigadzira 'zvakaremara' muchigadzirwa, zvichitungamira kuparara kwekutanga kwemuenzaniso, uye nokudaro kuderedza kuparara kwekuita kwemuenzaniso.


4. Pesvedzero yekugadzira fomula pane kuparara kwesimba


Kugadzirisa fomula ndicho chinongedzo chakakosha mukugadziriswa kwezvigadzirwa zveEPDM kuita zvigadzirwa zvemagetsi ekudzivirira, asiwo chimwe chezvinhu zvakakosha zvinokanganisa kuparara kwezvigadzirwa zvemagetsi ekudzivirira. Kugadziriswa uye optimization yeiyo yekutanga kugadzirisa fomula uye kuwedzera kwemagetsi insulating additives kunogona zvakanyanya kuvandudza kuparara kwekuita kwemagetsi ekudzivirira zvigadzirwa. Mushure mokunge EPDM imwechete yakasvibiswa inoshandiswa maererano nemhando dzakasiyana-siyana, maitiro emagetsi haashanduki zvakanyanya, uye iyo yekupedzisira inongova inenge 5% yakakwirira kudarika yekare, asi simba rekuputsika kwemagetsi rine kuchinja kukuru, uye iyo yekupedzisira inenge 60% yakakwirira kupfuura yekare. Chikonzero chikuru chekuvandudzwa kwemakanika nemagetsi zvinhu ndechekuti mugadziri wetambo dzemugungwa akakwenenzvera dosage ye diisopropyl benzene peroxide panguva yekugadzirwa kwezvinhu, kuitira kuti mabhondi maviri ari mumativi eketani eENB anyatsopindirana, uye akasara maviri mabhondi anoderedzwa, uye kaolin nemamwe magetsi ekudzivirira emagetsi anowedzerwa, ayo anogona kuwedzera dhizaini uye yakasara. zvigadzirwa. Aya mapoinzi maviri ari pamusoro akakwana kuratidza kukosha kweiyo fomula yekugadziridza yekuvandudza kuparara kwemagetsi kushanda kweEPDM magetsi ekudzivirira zvigadzirwa.


5. Mhedziso

(1) Iyo yakapetwa kaviri chisungo mucheni yepadivi chetatu monoma (ENB) muEPDM inokwana zvakakwana kuyambuka-yakabatana.

(1) EPDM mune yechitatu monomer (ENB) mucheni yeparutivi yechisungo cheviri, iyo yakanyanya kuyambuka-yakabatana, iyo yakaderera nhamba yezvisaririra, iyo inonyanya kubatsira kune magetsi ekudzivirira zvigadzirwa (waya uye tambo yekuvharisa) yemagetsi kuputsika kuramba kuita.

(2) Iyo yakakwirira kuchena kweEPDM raw material (iyo yakaderera madota), iyo inonyanya kubatsira pakuvandudzwa kwemagetsi ekudzivirira zvigadzirwa (waya uye cable insulation layer) yemagetsi kuputsika kuramba.

(3) Iyo yakaderera iyo gel yemukati yeEPDM mbishi zvinhu, iyo inonyanya kubatsira kuvandudza emagetsi ekudzivirira zvigadzirwa (waya uye tambo yekuvharisa) yemagetsi kuputsika kuramba.

(3) Iyo yakaderera iyo gel yemukati yeEPDM mbishi zvinhu, zviri nani kuparara kwekupokana kwemagetsi ekudzivirira zvigadzirwa (waya uye tambo yekuvharisa).

(4) Kugadzirisa huwandu hweEPDM mukugadzirwa kwechigadziko chemagetsi insulators (waya uye tambo yekuvharisa) uye kuiwedzera nemagetsi ekudzivirira emagetsi ekuwedzera anogona kuvandudza zvakanyanya kuparara kwekupokana kwemagetsi insulators (waya uye tambo yekuvharisa).


KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.