Qodobbada saameeya caabbinta burburka ee fiilada caagga ah ee ethylene propylene iyo lakabka daboolka fiilada

Aragtida: 0     Qore: Tifaftiraha Goobta Waqtiga Daabacaadda: 2023-08-13 Asal ahaan: Goobta

Weydiiso

Marka loo eego ethylene, propylene iyo diolefin aan isku xidhnayn kobolymerization ethylene propylene diene caag (EPDM) sida silig iyo qalabka dahaadhid cable ay leeyihiin in ka badan 60 sano oo taariikhi ah. EPDM iyo polyvinyl chloride (PVC) iyo polyetylen-ku-xiran (XLPE) iyo walxaha kale ee dahaadhka ah waxay leeyihiin boos isku mid ah oo aan la bedeli karin, faa'iidooyinkeeda gaarka ah waa: nolosha adeegga oo dheer, caabbinta wanaagsan ee biyaha iyo ogsijiinta iyo xasilloonida kulaylka, heerkul ballaadhan oo heerkul ah. Maaddaama codsiga EPDM ee duurka korantada korantada ay aad iyo aad u ballaaran tahay, shuruudaha tilmaamayaasha muhiimka ah ee EPDM ayaa sidoo kale aad u baahan, gaar ahaan codsiyada dhamaadka-sare qaarkood, xakamaynta tilmaamayaasha muhiimka ah ee EPDM waxay leedahay shuruudo adag, kaliya marka tilmaamayaasha muhiimka ah ee u dhigma ay ku jiraan qiyaas macquul ah, si EPDM ay u buuxiso habka, waxqabadka iyo isticmaalka shuruudaha. Qaado EPDM tusaale ahaan soo saarista silig-voltage-ka dhexe iyo dahaarka fiilada, haddii xoogga jilicsanaanta, dhererka dillaaca, xoogga burburka, lumista dielectric, caabbinta mugga iyo sifooyinka kale ee muhiimka ah ee farsamada iyo korantada ee alaabta ayaa buuxin kara shuruudaha, walxaha EPDM ethylene alaabta ceeriin, mooney viscosity, content diolefin iyo daahirnimada iyo tilmaamayaasha kale ee muhiimka ah waa inay lahaadaan xaddidaad adag. Waxaa jira arrimo badan oo saameeya caabbinta jabka ee siliga EPDM iyo dahaarka fiilada. Marka lagu daro nuxurka ethylene ee kor ku xusan, maadada diolefin iyo nadiifinta, maadada jel ee EPDM, iyo sidoo kale hagaajinta iyo hagaajinta habka wax-qabadka ayaa saameyn muhiim ah ku leh caabbinta burburka alaabta. Ma aha oo kaliya hal iyo arrimo saameyn leh, laakiin sidoo kale waxay wada shaqeeyaan si ay u yeeshaan saameyn dhamaystiran oo ku saabsan caabbinta burburka korantada ee alaabta. Warqadan, qaar ka mid ah arrimaha saameeya caabbinta burburka ee EPDM ayaa loo xushay cilmi baaris iyo falanqeyn nidaamsan, si loo bixiyo tixraac muhiim ah oo loogu talagalay isku dhafka alaabta EPDM ee xargaha iyo xargaha xargaha.


1 Saamaynta nuxurka ENB ee xoogga burburka


Waxyaabaha ku jira ENB (jajab tiro) <4.5%, iyo korodhka ENB-ga ku jira, awoodda burburka ee badeecadu way yaraataa; Waxyaabaha ku jira ENB (jajab tiro) ≥4.5%, iyo kororka maadada ENB (jajab tiro), awoodda burburka ee badeecadu way korodhaa.


2. Saamaynta nadiifinta caagga ah ee xoogga burburka


Marka EPDM loo isticmaalo habaynta walxaha dahaadhka korantada, nadiifinta walxaha ayaa loo baahan yahay ilaa xad. Nadiifinta EPDM waxaa badanaa lagu muujiyaa nuxurka dambaska, taas oo inta badan ka kooban milix aan dabiici ahayn oo ay ku jiraan ion bir ah (vanadium, aluminium, iron, sodium, iwm.) oo la soo galiyay inta lagu jiro polymerization iyo ka-dib-u-socodka, iyo sidoo kale wasakh shisheeye. Jiritaanka dambaska, oo u dhiganta 'cilad' jireed, si fudud u noqota horumar ku saabsan alaabta caagga ah ee koronto. Marka maaddada dambaska ee EPDM ay korodho, waxa ku jira ion birta ee muunada sidoo kale way korodhaa, iyo awoodda burburka ee alaabta la dhammeeyey ayaa hoos u dhacda. Ash (Iyoon bir, wasakh shisheeye) waxay saamayn gaar ah ku leeyihiin waxqabadka burburka korantada ee alaabta. Iyadoo la tixgelinayo saameynta ion birta ee caabbinta burburka ee badeecada, ions birta ee muunada tijaabada waxay sameyn doonaan beer gudaha ah oo gudaha ah oo hoos timaada ficilka beerta koronto ee dibadda, kaas oo lagu dhejin doono goobta dibadda si ay u dhaawacdo alaabta. Marka maaddada ion birta ee muunada ay kordho, xoogga gudaha gudaha ayaa si tartiib tartiib ah u kordheysa, suurtagalnimada isugeynta gudaha ee ions birta ayaa sidoo kale kor u kacda, taasoo keentay in aan caadi ahayn oo xoog leh oo degaanka ah, dhammaan arrimahan ayaa yareyn doona caabbinta burburka alaabta. Marka labaad, ka fiirso saamaynta ay wasakhda shisheeye on caabbinta burburka ee alaabta, alaabta caag ah ee nijaasta shisheeye inta badan waxaa ka mid ah ciid iyo miridhku, iwm, sida caadiga ah, wasakhda iyo caag, kuwaas oo waafaqid aad u liidata, iyo joogitaanka alaabta caag ah oo u dhiganta a 'cilad' ah, burburinta isku midka ah iyo daacadnimada alaabta caag ah. Marka garoon koronto oo sare oo koronto ah uu ku shaqeeyo EPDM alaabada dahaarka korantada ee leh 'ciladaha', waxay ahaan doontaa ilaa xad fudud in la jebiyo alaabta dahaarka korantada ee 'ciladaadka', sidaas darteed hoos u dhigista caabbinta alaabta ee burburka korontada.


3. Saamaynta maadada jelka ee xoogga burburka


Jeelku waa qaab-dhismeed gaar ah oo ah 'qurub caag ah' oo la sameeyay intii lagu jiray polymerization of EPDM. Qaab-dhismeedkeeda gaarka ah iyo qaab-dhismeedkeeda awgeed, is-dhexgalka ay la leedahay silsiladda molecular ee caadiga ah ee alaabta caagga ah ayaa ah mid daciif ah, jiritaankeedana waxaa sidoo kale loo arki karaa 'nijaasnimo' oo ku hartay alaabta caagga ah. 'Waxyaalaha tayada sare leh ee EPDM alaabada dahaarka korantada, maadada jelku waxay sidoo kale saameyn ku yeelan kartaa waxqabadka burburka korantada ee alaabta. Sida maadada jel ee EPDM kor u kacdo, xoogga burburka ee alaabta la dhammeeyey ayaa hoos u dhacda. Maadaama jelku yahay qaab-dhismeedka mesh-ka ah ee isku-dhafan, qaab-dhismeedkiisu aad ayuu uga duwan yahay kan caadiga ah ee silsiladaha EPDM molecular EPDM, sidaas darteed waa mid aan la jaan qaadi karin silsiladaha EPDM ee caadiga ah marka loo eego molecular EP dhexgalka u dhexeeya dusha jel iyo silsiladaha kelli ee caadiga ah waa ka daciifsan yahay inta u dhaxaysa silsiladaha molecular ee caadiga ah ee EPDM.


Dusha sare ee jelku qasab maaha in 'ka buuxsamo' silsiladaha unugyada EPDM, waxaana laga yaabaa inay jiraan qaar ' nusqaamooyin' ah. Maaddaama jiritaanka jelku uu saameyn doono isku-noolaanshaha sheyga, badeecada la warshadeeyay waxay sameyn doontaa jaangooyooyin beer ah oo ku wareegsan jel iyada oo la raacayo ficilka bannaanka sare ee korantada. Farqiga weyn ee u dhexeeya qaab-dhismeedka iyo qaab-dhismeedka jel-ka iyo silsiladaha molecular ee ku xeeran ee EPDM, way sii weynaanaysaa samaynta jaan-goynta goobta, way fududahay in la jebiyo dusha sare ee jel kaas oo leh awood qaraabo ah oo daciif ah waxaana laga yaabaa in 'farqi' ku dhex jiro alaabta. Inta badan farqiga u dhexeeya silsiladaha molecular ee EPDM, ayaa sii weynaanaya qulqulka beerta, waxay u badan tahay inay burburiyaan dusha jel halkaasoo xoogga qaraabada ah uu daciif yahay waxaana laga yaabaa inay jiraan ' nusqaamo ' ee alaabta, taasoo horseedaysa burburka hore ee muunada, oo sidaas awgeed hoos u dhigaya waxqabadka burburka ee muunada.


4. Saamaynta caanaha habaynta ee xoogga burburka


Habka habaynta ayaa ah isku xidhka furaha u ah habaynta alaabta EPDM ee alaabada dahaadhka korantada, laakiin sidoo kale waa mid ka mid ah qodobbada muhiimka ah ee saameeya burburka waxqabadka alaabta korantada. Hagaajinta iyo hagaajinta habka aasaasiga ah ee wax-soo-saarka iyo ku-darka waxyaabaha lagu daro korantada korantada waxay si weyn u wanaajin kartaa burburka alaabta korantada. Ka dib markii isla alaabta ceeriin ee EPDM loo habeeyo si waafaqsan qaabab kala duwan, sifooyinka farsamada wax badan ma beddelaan, kan dambena wuxuu ku saabsan yahay 5% oo keliya ka sarreeya kii hore, laakiin xoogga burburka korantada ayaa leh isbeddel weyn, kan dambena wuxuu ku saabsan yahay 60% ka sarreeya kii hore. Sababta ugu weyn ee hagaajinta guryaha makaanikada iyo korantada ayaa ah in soo saaraha fiilada badda uu hagaajiyay qiyaasta diisopropyl benzene peroxide inta lagu gudajiro wax soo saarka, si labada bond ee silsiladda dhinac ee ENB ay si buuxda isugu xirmaan, iyo bonds double haraaga ah ayaa la dhimay, iyo kaolin iyo daroogooyinka kale ee korantada ee kale ayaa lagu daray, taas oo kordhisa wax soo saarka iyo wax soo saarka ee dusha sare. Labada dhibcood ee kor ku xusan waxay ku filan yihiin inay caddeeyaan muhiimada qaacidada farsamaynta si loo hagaajiyo waxqabadka burburka korantada ee alaabta dahaarka korantada ee EPDM.


5.Gabagabadii

(1) Isku-xidhka labanlaabka ah ee silsiladda dhinaca ee monomer-ka saddexaad (ENB) ee EPDM ayaa si ku filan isugu xiran.

(1) EPDM ee monomer-ka saddexaad (ENB) ee silsiladda dhinaca ee isku-xidhka laba-jibbaaran, si buuxda oo iskutallaab ah, hoos u dhaca tirada haraaga, wax badan oo ku habboon alaabooyinka korantada korantada (siliga iyo xargaha xargaha) waxqabadka caabbinta korantada.

(2) Nadiifadda sare ee alaabta ceyriinka ah ee EPDM (hoos u kaca maadada dambaska), ayaa aad waxtar u leh hagaajinta alaabta korantada korantada (lakabka dahaadhka fiilada iyo fiilada) caabbinta burburka korantada.

(3) Mawduuca jel-ka hoose ee alaabta ceeriin ee EPDM, ayaa wax badan ka caawinaysa hagaajinta alaabta korantada korantada (siliga iyo xargaha xargaha) caabbinta burburka korontada.

(3) Mawduuca jel-ka hoose ee alaabta ceeriin ee EPDM, ayaa si fiican u caabbinta burburka alaabada korantada (xadhkaha iyo fiilada).

(4) Hagaajinta qadarka EPDM ee aasaaska aasaasiga ah ee dahaarka korantada (xadhkaha fiilada iyo fiilada) iyo ku-darka waxyaabaha lagu daro korantada korantada waxay si weyn u wanaajin kartaa caabbinta burburka dahaadhka korantada (xadhkaha fiilada iyo fiilada).


XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.