Ethylene propylene rabara (haholo-holo binary ethylene propylene rabara) e sebelisoa ka bongata e le viscosity index modifier (OVI kapa VII) bakeng sa oli e mengata ea hydrocarbon ho ntlafatsa lubricity ea oli mochesong o phahameng le o tlase le ho etsa hore oli e sebetse betere maemong a tsitsitseng le a matla.
Ethylene propylene rabara e hloka matla a phahameng a teteaneng, ntlha e tlaase ea ho tšela le index e tlaase ea ho kuta ha e sebelisoa e le sehlomathiso sa mofetoleli bakeng sa lubricant, peterole le diesel.
Khothalletsa:
EPDM:CO 033;CO 034;CO 043;CO 054;