Yakakwirira-Simba Oiri-Inopikisa Medium-Saturation HNBR Synthetic Rubber
Mhedziso Yechigadzirwa: Yakakwirira-Simba Oiri-Inodzivirira Medium-Saturation HNBR Synthetic Rubber
Yedu Yepakati-Saturation HNBR Synthetic Rubber yakagadzirwa kuti ibudise kuita kwakasiyana-siyana munzvimbo dzakafumurwa oiri uye dzakanyanya kushushikana mumaindasitiri. Iine 34% acrylonitrile yemukati, iyi hydrogenated nitrile rubber (HNBR) inopa yakakwirira mafuta kuramba ichiramba ichichinjika uye kusimba, ichiita kuti ive yakanakira zvisimbiso, gaskets, uye zvikamu mumamiriro ekushanda akaomarara.
Yakakosha Tekinoroji Madiro:
- Acrylonitrile Zvemukati: 34% - Yakagadziridzwa yekuenzanisa mafuta kuramba uye yakaderera-yekushisa kuchinjika.
-Mooney Viscosity (ML 1+4 @125°C): 70-90 - Inopa yakanakisa processability yekuumba uye extrusion.
-Iodine Absorption Value: 11-22 - Inoratidza inodzorwa yepakati saturation yekuwedzera kugadzikana kwemakemikari uye kuramba kuchembera.
- Kuoma: Inogadziriswa renji (semuenzaniso, 60-90 Shore A) kusangana nemhando dzakasiyana dzekushandisa.