Properties:
Kunyanya kupisa kwekushisa (-20 ° C kusvika +250 ° C).
Kupokana kwakasarudzika kumafuta, mafuta, zvinonyungudutsa, acids, uye mabhesi.
High tensile simba (10-20 MPa), low compression set (<15% pa 150 ° C / 70h).
Flame retardant (UL94 V-0 rating) uye ozone-resistant.
Zvakanakira:
Pre-yakasanganiswa nemishonga (semuenzaniso, bisphenol AF, peroxide) kuitira vulcanization inoshanda.
Inochengetedza kugadzikana kwedimensional munzvimbo dzine hukasha dzemakemikari.
FDA-inoenderana mamakisi anowanikwa kune chikafu / yekurapa kuonana.
Applications:
Aerospace: Fuel system O-mhete, zvisimbiso zveinjini, uye diaphragms.
Motokari: Turbocharger gaskets, transmission seals, uye majekiseni emafuta.
Kemikari: Pombi linings, zvigaro zvevharuvhu, uye hose assemblies.
Properties:
Kupisa kupisa kusvika +150 ° C (inopindirana +175 ° C).
Kunyanya kupikisa mafuta, amines, uye hydraulic fluids.
High tensile simba (15-35 MPa) uye kuneta kuramba.
Low permeability kune magasi.
Zvakanakira:
Pre-vulcanized yekuderedzwa yekugadzirisa nguva.
Inochengetedza elasticity pasi pekuratidzwa kwenguva refu kune hutsinye media.
Inowanikwa muperoxide- kana sulfur-cured grade.
Applications:
Oiri & Gasi: Kuchera mapaketi, madhaka pombi zvisimbiso, uye zvikamu zvetsime.
Motokari: Mabhandi enguva, majekiseni emafuta, uye turbocharger hoses.
Indasitiri: Hydraulic cylinder seals uye gearbox zvikamu.
Properties:
Pakati pemafuta kuramba (zviri nani pane EPDM, isingasviki HNBR).
Tembiricha yakasiyana: -40°C kusvika +120°C.
High abrasion resistance (ASTM D5963: 100–200 mm³ kurasikirwa).
Good resilience uye compression set resistance.
Zvakanakira:
Inodhura-inoshanda nekuumbwa kwakanakisa.
Customizable acrylonitrile yemukati (18-50%) yeyakagadzirirwa mafuta kuramba.
Applications:
Motokari: Mapaipi emafuta, O-mhete, uye zvisimbiso zvekutumira.
Indasitiri: Mabhandi ekutakurisa, ma roller ekudhinda, uye zvisimbiso zve hydraulic.
Mutengi: Latex magurovhosi nemidziyo yemitambo.
Properties:
Yakasarudzika ozone / yemamiriro ekunze kuramba (5,000+ maawa mukuyedzwa kweQUV).
Kupisa: -50 ° C kusvika +150 ° C.
High dielectric simba (20-30 kV/mm) uye kusamira kwemvura.
Low gasi permeability.
Zvakanakira:
Pre-yakagadzirwa ne antioxidants uye UV stabilizers.
Yakanakisa vibration damping (kurasikirwa chinhu: 0.1-0.3).
Applications:
Motokari: Zvisimbiso zvegonhi, hosi dzeradiyeta, uye mamongi einjini.
Kuvaka: Mamembrane edenga, mabhandi emadziva, uye gaskets dzemahwindo.
Electrical: Cable insulation uye mabhandi ekufambisa simba.
Properties:
High tensile simba (20-60 MPa) uye elasticity (kusvika 800% elongation).
Kusarudzika abrasion kuramba (ASTM D5963: 20-50 mm³ kurasikirwa).
Tembiricha yemhando: -40 ° C kusvika +100 ° C (kusvika + 120 ° C ine kupisa stabilizers).
Inopikisa kune solvents uye hydrolysis.
Zvakanakira:
Customizable kuoma (Shore A 50–95).
Inowanikwa mu cast, millable, kana thermoplastic mamakisi.
Applications:
Indasitiri: Mavhiri, rollers, uye mabhandi ekutakura.
Motokari: Suspension bushings, shock absorbers, uye CV joint boots.
Kurapa: Catheters, simbi dzemapfupa, uye prosthetics.
Properties:
Kuramba kuchipisa kupisa kusvika +150 ° C (kupindirana +175 ° C).
Yakanakisa kuramba kune otomatiki transmission fluid (ATF), oiri, uye kupisa.
Moderate ozone uye kuramba mamiriro ekunze.
Kusimba kwesimba: 7–15 MPa.
Zvakanakira:
Pre-yakasanganiswa neamine kana peroxide mishonga yekurapa nekukurumidza.
Inochengetedza kugadzikana kwedimensional munzvimbo dzeATF.
Applications:
Motokari: Zvisimbiso zvekutumira, O-mhete, uye madiaphragms epombi.
Power steering system zvikamu.
Indasitiri: Pombi zvisimbiso zvemafuta-based media.
Properties:
Wide tembiricha range (-40°C kusvika +150°C).
Kupokana nemafuta, glycols, uye mamiriro ekunze.
High tensile simba (10-20 MPa) uye compression set kuramba.
Low permeability kune magasi.
Zvakanakira:
Kuenzanisa kupisa kusagadzikana uye kushanduka.
Inopesana ne hydrolysis uye kuchembera.
Inowanikwa muperoxide- kana sulfur-cured grade.
Applications:
Motokari: Radiator hoses, inotonhorera system zvikamu, uye mahosi ekupinda mhepo.
Indasitiri: Mabhandi ekutakurisa emakemikari ekubata uye madiaphragms epombi.
HVAC: Duct gaskets uye vibration isolators.