Ɔhaw ahorow a ɛtaa ba ne ano aduru a wɔde yɛ rɔba timing belt ho nsɛm tiawa

Point 1. Synchronous belt a ɛpaapae ntɛm

1. Wɔnsusuw inertia force a ɛwɔ driven wheel ne driven load no ho.

2、 Adesoa no sõ dodo anaasɛ passive wheel no gyina esiane akwanhyia nti, na ɛnam so ma adesoa ahoɔden no kɔ soro kɛse.

3、Pulley no sua dodo na wɔde ahoɔden abɔ abɔso no so.

Anoyie:

1、Ma nhyehyɛe no tu mpɔn.

2. Hwɛ sɛnea wɔayɛ no na fa nea ɛwɔ sẽ pii sen nea ɛba fam koraa no si pulley no ananmu.

3, ɛsɛ sɛ wohu sɛnea wodi ho dwuma, wɔkora so, wɔhyehyɛ ne sɛnea wɔyɛ no yiye na wɔhwɛ yiye.



Point 2. Synchronous abɔso abɔso ano a ɛyɛ mmerɛw

1、Wɔmma ntwahonan no nsɛso ho kwan.

2、Insufficient bearing kateeyɛ.

3、Bending a ɛwɔ retaining ano a ɛwɔ belt wheel no mu.

4、Pulley no ntwemu sua sen abɔso no trɛw.

Anoyie:

1、Calibrate gyinabea a ɛwɔ pulley no.

2、Ma rigidity a bearing no yɛ kɛse na siesie no denneennen.

3、Teɛɛ retaining edge anaa sesa.

4. Hwɛ sɛnea wɔayɛ no.


Point 3.Synchronous abɔso sẽ soro wear

1、Adesoa no sõ dodo.

2、Belt tensioning tumi yɛ kɛse dodo.

3、Adulterated abrasive powder a wɔde ahyɛ mu.

4、Rough ntwahonan sẽ.

Anoyie:

1、Ma nhyehyɛe no tu mpɔn.

2、Sesa abɔso tensioning tumi.

3、Ma nneɛma a atwa yɛn ho ahyia no tu mpɔn na ma ahobammɔ kataso no nkɔ soro.

4、Siesie hann ntwahonan sẽ anaa sesa pulley.


Point 4. Synchronous belt sẽ no mu paapae

1、Nse a wɔahuruw.

2. Passive mfiri akwanhyia adesoa kɔ soro.

Anoyie:

1. Hwɛ sɛnea wɔayɛ no.

2、Sesa tumi a ɛfata a wɔde hyɛ mu.

3、Ma pulley no ntwemu nkɔ soro na ma sẽ dodow nkɔ soro.

4、Fa passive mfiri huammɔdi fi mu


Point 5. Synchronous belt a rɔba akyi asɛe na ɛpaapae

1、Abɔnten so tensioning wheel rotation no yɛ nea wɔasiw ano.

2、Abɔnten so nhyɛso ntwahonan misalignment.

3. Nhyia mfiri no frame.

4、bere tenten a ɛba fam ɔhyew tebea.

Anoyie:

1、Siesie anaa sesa tension wheel bearings no.

2、Teɛɛ tension wheel gyinabea.

3、Hwɛ na teɛteɛ mfiri afã horow no.

4、Ma ambient temperature tu mpɔn.


Point 6. Softening a ɛwɔ akyi.

1、Ɔhyew a ɛkorɔn

2、Tensioning ntwahonan gyinabea.

3、Ngo a ɛyɛ nnam.

Anoyie:

1、Ma ambient temperature tu mpɔn.

2、Hwɛ na siesie tensioning wheel no.

3、Nbata ngo ho anaasɛ nsakra ngo a ɛko tia synchronous belt no.


Point 7. Belt tenten mu mpaapaemu

1、Timing belt no tu mmirika kɔ akyiri sen pulley no ano.

2、Synchronous abɔso rolls kɔ soro retaining ano a pulley no.

Anoyie:

1、Sesa gyinabea a belt pulley no wɔ.

2、Enhance bearing rigidity na siesie pintinn.


Point 8. Nipadua fã a ɛtwetwe no a abubu

1、Nneɛma a ɛnteɛ loading ne unloading timing belt.

2, a wɔde afrafra nneɛma a asɛe anaasɛ nkae a ano yɛ nnam na ano yɛ nnam.

Anoyie:

1、Ɔkwan a ɛteɛ a wɔfa so de nneɛma gu mu na woyi synchronous belt.

2、Ma nneɛma a atwa yɛn ho ahyia no tu mpɔn. Fa akatasoɔ a ɛbɔ ho ban ka ho.


Point 9. Dede a ɛdɔɔso dodo bere a woretu mmirika no

1、Tensioning tumi a synchronous belt yɛ kɛse dodo.

2. Parallel misalignment a ɛwɔ agyan abien no mu.

3、Timing belt no trɛw yɛ kɛse sen pulley no ntwemu.

4、Adesoa no sõ dodo.

5、Timing belt ne pulley sẽ no hyɛ yiye.

Anoyie:

1、Sian tensioning wheel (no ahuru sẽ nni nkonim).

2、Sesa gyinabea a ɛwɔ belt pulley no.

3、Ma nhyehyɛe no tu mpɔn.

4、Ma nhyehyɛe no tu mpɔn.

5、Hwɛ timing belt ne pulley.


Point 10.Belt pulley sẽ wear

1、Adesoa no sõ dodo.

2、Nhyɛso a ɛwɔ synchronous belt mu no yɛ kɛse dodo.

3、Adeɛ a wɔde yɛ pulley no nyɛ papa.

4、Mfutuma a ɛyɛ abrasive a wɔde afrafra.

Anoyie:

1、Ma nhyehyɛe no tu mpɔn.

2、Bɔ fam tumi a ɛma nhyɛso no.

3、Fa nneɛma a ɛyɛ den a ɛwɔ hardening ayaresa wɔ soro.

4、Ma nneɛma a atwa yɛn ho ahyia no tu mpɔn na ma ahobammɔ kataso no nkɔ soro.



NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.