Muli pano: Kunyumba » Zothetsera » Chidule cha mavuto omwe anthu ambiri Zothetsera amakumana nawo ndi mayankho a lamba wanthawi ya rabara

Chidule cha zovuta zomwe wamba ndi njira zothetsera lamba wanthawi ya rabara

Mfundo 1. Kuthyoka koyambirira kwa lamba wa synchronous

1. Mphamvu ya inertia ya gudumu loyendetsedwa ndi katundu woyendetsedwa sizikuganiziridwa.

2, Katunduyo ndi wamkulu kwambiri kapena gudumu loyima limayima chifukwa cha ngozi, motero kumawonjezera mphamvu yolemetsa.

3, Pulley ndi yaying'ono kwambiri ndipo lamba amapindika mokakamiza.

Yankho:

1, Sinthani mapangidwe.

2. Yang'anani kapangidwe kake ndikusintha pulley ndi imodzi yokhala ndi mano ambiri kuposa yochepera yoyambira.

3, kusamalira, kusungirako, kukhazikitsa ndi kugwiritsa ntchito kuyenera kukhala odziwa bwino komanso osamala.



Mfundo 2. Synchronous lamba m'mphepete kuvala

1, Kufanana kwa gudumu sikuloledwa.

2, Kusakwanira kubereka kukhazikika.

3, Kupindika kwa m'mphepete mwa gudumu lamba.

4, The awiri a pulley ndi yaying'ono kuposa m'lifupi lamba.

Yankho:

1, Sinthani malo a pulley.

2, Wonjezerani kukhazikika kwa chonyamulira ndikuchikonza mwamphamvu.

3, Konzani chosungirako kapena m'malo mwake.

4. Yang'anani kapangidwe kake.


Point 3.Synchronous lamba dzino pamwamba kuvala

1, Katunduyo ndi waukulu kwambiri.

2, Mphamvu yolimbitsa lamba ndi yayikulu kwambiri.

3, Wosanjikiza ufa wonyezimira.

4, Mano olimba.

Yankho:

1, Sinthani mapangidwe.

2, Sinthani mphamvu yolimbitsa lamba.

3, Sinthani chilengedwe ndikuwonjezera chivundikiro choteteza.

4, Konzani mano gudumu kuwala kapena kusintha pulley.


Mfundo 4. Mano a lamba wa synchronous amathyoka

1, Mano akulumpha.

2. Kuchulukirachulukira kwangozi kwamakina kumawonjezeka.

Yankho:

1. Yang'anani kapangidwe kake.

2, Sinthani mphamvu yolimbikitsira yoyenera.

3, Wonjezerani kukula kwa pulley ndikuwonjezera kuchuluka kwa mano.

4, Kupatula kulephera kwamawotchi


Mfundo 5. Lamba wa Synchronous wokhala ndi mphira kumbuyo kuvala ndi kusweka

1, Kuzungulira kwa gudumu lakunja kwatsekedwa.

2, Kusokoneza gudumu lakunja.

3. Kukumana ndi chimango cha makina.

4, Yaitali otsika kutentha boma.

Yankho:

1, Konzani kapena kusintha mayendedwe gudumu mavuto.

2, Konzani gudumu lamphamvu.

3, Chongani ndi kukonza mbali makina.

4, Sinthani kutentha yozungulira.


Mfundo 6. Kufewetsa ndi kuthandizira.

1, Kutentha kwakukulu

2, Kuyimitsa gudumu loyimitsa.

3, Mafuta omata.

Yankho:

1, Sinthani kutentha yozungulira.

2, Chongani ndi kusintha tensioning gudumu.

3, Osamamatira ku mafuta kapena kusintha lamba wosamva mafuta.


Mfundo 7. Lamba longitudinal akulimbana

1, Lamba wanthawi yake amadutsa m'mphepete mwa pulley.

2, Lamba wa Synchronous amagudubuza m'mphepete mwa pulley.

Yankho:

1, Sinthani malo a pulley lamba.

2, Limbikitsani kukhazikika ndikuwongolera mwamphamvu.


Mfundo 8. Kuthyoka kwa gawo lolimba la thupi

1, Kutsitsa kolakwika ndikutsitsa lamba wanthawi.

2, yosakanikirana ndi zinyalala kapena zotsalira zakuthwa komanso zakuthwa.

Yankho:

1, Njira yolondola yotsitsa ndi kutsitsa lamba wa synchronous.

2, Kupititsa patsogolo chilengedwe. Onjezerani chitetezo.


Mfundo 9. Phokoso lambiri mukathamanga

1, Mphamvu yolimba ya lamba wa synchronous ndi yayikulu kwambiri.

2. Kulumikizana molakwika kwa nkhwangwa ziwiri.

3, M'lifupi lamba wa nthawi ndi wamkulu kuposa awiri a pulley.

4, Katunduyo ndi waukulu kwambiri.

5, Lamba wanthawi ndi mano a pulley sakwanira bwino.

Yankho:

1, Tsitsani gudumu lolimba (palibe mano odumphira).

2, Sinthani malo a pulley lamba.

3, Sinthani mapangidwe.

4, Sinthani kapangidwe.

5, Onani lamba wanthawi ndi pulley.


Point 10.Belt pulley dzino kuvala

1, Katunduyo ndi waukulu kwambiri.

2, Kuvuta kwa lamba wa synchronous ndikokulirapo.

3, Zinthu za pulley si zabwino.

4, Chigololo cha fumbi la abrasive.

Yankho:

1, Sinthani mapangidwe.

2. Chepetsani mphamvu yamphamvu.

3, Gwiritsani ntchito zinthu zolimba ndi mankhwala owumitsa pamwamba.

4, Sinthani chilengedwe ndikuwonjezera chivundikiro choteteza.



MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.