Takaitacciyar matsalolin gama gari da mafita don bel na lokaci na roba

Ma'ana 1. Farkon karaya na bel na aiki tare

1. Ba a la'akari da ƙarfin rashin ƙarfi na motar motsa jiki da nauyin da aka yi amfani da shi.

2. The load ne da yawa girma ko m dabaran tsaya saboda wani hatsari, don haka ƙwarai ƙara load karfi.

3. Jul ɗin ya yi ƙanƙara kuma an lanƙwasa bel ɗin da karfi.

Magani:

1. Inganta zane.

2. Bincika ƙira kuma maye gurbin jakunkuna tare da ɗaya tare da ƙarin hakora fiye da mafi ƙarancin asali.

3, handling, ajiya, shigarwa da kuma aiki ya kamata a cikakken sani da kuma a hankali.



Ma'ana 2. Daidaitawar bel gefen bel

1. Ba a yarda da daidaiton dabaran ba.

2. Rashin isasshen ƙarfi.

3. Lankwasawa na riƙe gefen dabaran bel.

4. A diamita na Puley ne karami fiye da nisa na bel.

Magani:

1. Daidaita matsayi na ja.

2. Ƙara rigidity na bearing da gyara shi da ƙarfi.

3. Gyara gefen riƙewa ko maye gurbin shi.

4. Duba zane.


Point 3.Madaidaicin bel ɗin hakori saman lalacewa

1.Load ɗin yayi girma da yawa.

2. Belt tensioning karfi ya yi yawa.

3. Adulterated abrasive foda Layer.

4. Hakora masu tauri.

Magani:

1. Inganta zane.

2. Daidaita bel tensioning karfi.

3. Inganta muhalli da haɓaka murfin kariya.

4. Gyara hakora masu haske ko canza ja.


Ma'ana 4. Haƙoran bel ɗin aiki tare suna karye

1. Tsallewar hakora.

2. M inji hatsari load yana ƙaruwa.

Magani:

1. Duba zane.

2. Daidaita ƙarfin tashin hankali da ya dace.

3. Ƙara diamita na jan hankali da ƙara yawan hakora.

4. Banda m inji gazawar


Ma'ana 5. bel ɗin aiki tare tare da goyan bayan roba da fasa

1. The waje tensioning dabaran juyawa aka katange.

2. Outer tensioning dabaran misalignment.

3. Haɗu da firam ɗin injin ɗin.

4. Dogon lokaci low zazzabi jihar.

Magani:

1. Gyara ko maye gurbin tashin hankali dabaran bearings.

2. Gyara tashin hankali dabaran matsayi.

3. Duba kuma gyara sassan injiniyoyi.

4. Inganta yanayin zafin jiki.


Ma'ana 6. Yin laushi tare da goyan baya.

1. High zafin jiki

2. Tasha dabarar tayar da hankali.

3.Mai danko.

Magani:

1. Inganta yanayin zafin jiki.

2. Duba kuma daidaita dabaran tashin hankali.

3. Kada ku tsaya ga man fetur ko canza bel ɗin da ke da tsayayyar mai.


Ma'ana 7. Belt a tsaye tsaga

1. bel ɗin lokaci yana tafiya bayan gefen abin wuya.

2. bel ɗin daidaitacce yana jujjuya gefen riƙon abin wuya.

Magani:

1. Daidaita matsayin bel.

2. Haɓaka rigidity mai ɗaukar nauyi kuma gyara da tabbaci.


Ma'ana 8. Ragewar sashin jiki mai ƙarfi

1.Loading da saukar da bel ba daidai ba.

2, gauraye da tarkace ko kaifi da kaifi.

Magani:

1. A daidai Hanyar loading da sauke synchronous bel.

2. Inganta muhalli. Ƙara murfin kariya.


Ma'ana 9. Yawan hayaniya lokacin gudu

1. Tensioning da karfi na synchronous bel ne babba.

2. Daidaitaccen daidaitawar gatura biyu.

3. The nisa na lokaci bel ne ya fi girma da diamita na Puley.

4.Load ɗin yayi girma da yawa.

5. bel na lokaci da haƙoran ja ba daidai ba.

Magani:

1. Rage da tensioning dabaran (ba tsalle hakora rinjaye).

2. Daidaita matsayi na bel ja.

3. Inganta zane.

4. Inganta zane.

5. Bincika bel ɗin lokaci da ƙwanƙwasa.


Ma'ana 10. Belt Puley hakori lalacewa

1.Load ɗin yayi girma da yawa.

2. A tashin hankali na synchronous bel ne ma girma.

3. Kayan kayan kwalliya ba shi da kyau.

4.Zina da kura.

Magani:

1. Inganta zane.

2. Rage ƙarfin tashin hankali.

3. Yi amfani da m abu tare da hardening magani a saman.

4. Inganta muhalli da haɓaka murfin kariya.



SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.