GA-9540
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175°C x 5min x 15MPa.
| Product parameters | ||||
| Product | GA-9540 |
GA-9550 | GA-9560 | GA-9570 |
| Appearance | Translucent | |||
| William plasticity |
155 |
200 |
220 |
250 |
| Hardness (ShoreA) |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.14 |
1.17 |
1.19 |
1.20 |
| Tensile strength (MPa) |
8.0 |
9.0 |
10.0 |
11.0 |
| Elongation(%) | 600 |
500 |
450 |
300 |
| Tear strength (kN/m) | 14 |
25 |
25 |
25 |