GA-95×0 High gajiya m silicone roba (HCR)

Aikace-aikace: dace don samar da maɓalli, da dai sauransu.
Maɓalli masu mahimmanci: ƙarfin ƙarfi, ƙarfin juriya mai ƙarfi, rayuwar sabis ɗin ya kai sau miliyan 10, ƙaddamar da amincin RoHS, REACH, da
  • GA-9540

  • Herchy

Samun FDA:
Yawan:

Gwaji: 1% na wakili mai warkarwa (manna 50% na DBPMH a cikin silicone danko), 175°C x 5min x 15MPa.


Siffofin samfur
Samfura GA-9540
GA-9550 GA-9560 GA-9570
Bayyanar Translucent
William plasticity
155
200
220
250
Hardness ( ShoreA)
40
50
60
70
Girma (g/cm3) 1.14
1.17
1.19
1.20
Ƙarfin ɗaure (MPa)

8.0
9.0
10.0
11.0
Tsawaita(%) 600
500
450
300
Ƙarfin hawaye (kN/m) 14
25
25
25









Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.