GA-95 × 0 Kutopa kwakukulu kwa mphira wa silicone (HCR)

Ntchito: oyenera kupanga mabatani, etc.
Zofunika kwambiri: kulimba kwakukulu, kulimba mtima kwambiri, moyo wautumiki umafika nthawi 10 miliyoni, perekani kutsimikizika kwa RoHS, REACH, ndi FDA
  • GA-9540

  • Herchy

Kupezeka:
Kuchuluka:

Mayeso: 1% ya mankhwala ochiritsira (50% phala la DBPMH mu chingamu cha silicone), 175 ° C x 5min x 15MPa.


Mankhwala magawo
Zogulitsa GA-9540
GA-9550 GA-9560 GA-9570
Maonekedwe Zowoneka bwino
William plasticity
155
200
220
250
Kuuma (ShoreA)
40
50
60
70
Kachulukidwe (g/cm3) 1.14
1.17
1.19
1.20
Mphamvu yamagetsi (MPa)

8.0
9.0
10.0
11.0
Kutalikira (%) 600
500
450
300
Mphamvu yamisozi (kN/m) 14
25
25
25









Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.