GA-95×0 Raba ya silicone leyi tiyeke ya ku karhala lokukulu (HCR) .

Xitirhisiwa: xi lulamerile ku humesa swikomba-nkarhi, na swin’wana.
Swihlawulekisi swa nkoka: matimba ya le henhla, ku tiyisela ka le henhla ka ku tlhelela endzhaku, vutomi bya vukorhokeri byi fika eka 10 wa timiliyoni ta minkarhi, ku hundza ku tiyisisiwa ka RoHS, REACH, na FDA
  • GA-9540

  • Herchy

Ku kumeka:
Nhlayo:

Xikambelo: 1% wa xiaki xo horisa (50% wa paste ya DBPMH eka silicone gum), 175°C x 5min x 15MPa.


Tipharamitha ta Xiendliwa .
Ximakiwa GA-9540
GA-9550 GA-9560 GA-9570
Xivumbeko Ku vonakala loku vonakaka
William vupulasitiki
155
200
220
250
Ku nonoka (ShoreA) .
40
50
60
70
Ku tsindziyela(g/cm3) . 1.14
1.17
1.19
1.20
Ku tiya ka ku koka (MPa) .

8.0
9.0
10.0
11.0
Ku leha(%) . 600
500
450
300
Matimba ya ku handzuka (kN/m) . 14
25
25
25









Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.